Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Bora Care causes glue adhesion issues??

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Bora Care causes glue adhesion issues??

8/29/13       
antonio

Earlier this year we came up with a policy to apply Bora Care termiticide to all of our plywood and hardwood that comes into our shop before we start working with it. Thing is, i notice for everything that has had the bora care applied to it, it seems to not allow the wood glue to penetrate it, it just kinda dries on the surface and you can peel it off like dry caulk in a matter of minutes. Has this ever happened to any of you? If so, how did you deal with it? Should i use a damp rag and wipe some of the dried up bora care that resides on the surface of the wood prior to applying glue? Or wood a good sanding with some 80 grit do the trick?

9/2/13       #2: Bora Care causes glue adhesion issu ...
bob

Not sure what prompted your company to start treating incoming materials in this manor. If this is even an accepted regional practice, maybe I am unaware. But I have never heard of anybody doing this so bear with me.

If your findings are that the Bora Care is indeed what is causing the adhesion problems.

My suggestion is to STOP using the Bora care. Find a better way to deal with whatever problem you were having, that does not contaminate your materials.

If you are having issues with sheet goods and kiln dried lumber coming in with wood boring insects it is time to find a new supplier.

Otherwise it sounds as if you may have been having issues in your building. If that is the case you need to hire a qualified exterminator, and get that remedied. It is probably also time to speak with an industry consultant with expertise in wood science, sawing/drying, and plant operation.

9/2/13       #3: Bora Care causes glue adhesion issu ...
antonio

We started using this treatment as a preventative measure against termites infesting wood before it goes out to customers. Yes we do have both sub subterranean & dry-wood termites , we can not tent the place as the landlord wont allow us to (long story) and yes we do have pro exterminators come in and spray what they can where they can, but they have told me until i tent the place there is no sure way to kill all existing termites,,,,, so the best i can do is treat the wood as it comes in. Bora care is supposed to stop termites from using the wood as a food source. I have been told by the manufacturers of the product that it will not cause problems with paints, varnishes etc. Which is why i am trying to find out from other woodworkers if they had this problem.

9/3/13       #4: Bora Care causes glue adhesion issu ...
Charles Member

Time to find a new building????

I agree with bob. STOP using a product that is causing problems.

It just sounds wrong that a landlord would prevent a tenant from protecting his business from such an issue. I know you said it is a "long story" but maybe it is time to find a new landlord, or buy your own building. (A side benefit: a building might be a good long-term investment as well.)

Until you solve the insect problem, your business, and livelihood, is obviously at risk. I wonder how much money you are spending (losing) on exterminators and Bora Care products. That can't be helping your bottom line. If word gets out to the public that your building is infested, your business might just drop to zero. Would you buy products with that type of risk?

9/3/13       #5: Bora Care causes glue adhesion issu ...
antonio

Hey guys, while i appreciate all of your advice and input, remember, the first post i made was to find out if anyone had issues with bora care , i did not state that i knew with any certainty that i was having issues with it but to see if any other users had any problems with it and if so how they counteracted it. The reason why the landlord cant tent the place is because our building is connected to his own which totals a VERY big building which = big bucks to tent. I also would have bought my own building by now if i could have but for the size building i need that would be expensive here,,, once again we live in the caribbean,,, one of those '''paradises''' where you pay top dollar for just a carboard box! The exterminators were a once or twice deal , as i said before they admitted that their spraying was not going to do much. Bora care, while pricey, covers alot of square footage. I can treat over 25 sheets with just one gallon. It can also increase my bottom line,, think about it, what client wouldnt want to hear that their cabinets were treated with the best insecticide on the market, prior to being constructed? So back to my original question, has anyone out there used this product and got adhesion issues with it? Maybe its not the product, but the way i apply it?

9/3/13       #6: Bora Care causes glue adhesion issu ...
Charles Member

antonio,

not trying to disagree with you. i understand the building issues.

however, i don't know what type of cabinets you are selling. i would probably not want to know that kitchen cabinets, where i am storing food and dishes, contain a pesticide of some kind.

maybe the culture is different where you are and folks accept, or even prefer, poisonous chemicals in their cabinets. i don't know.

9/3/13       #7: Bora Care causes glue adhesion issu ...
Kilgore Trout Member

The Caribbean does have serious termite issues with any wood product. Practically all construction is masonry or metal - no wood will last if exposed.

I assume (big assumption) that most people will accept some degree of 'preventative measures' - toxicity - in their cabinets if that is the norm. But also a selling point that is a negative perhaps?

I think prevention is the first objective - Antonio needs to remove all termites from the premises so he does not contribute to the problem. That apparently is the crux of the problem, and until he moves, he will not be able to get a handle on it.

I would think that any buyer would prefer no Bora-care treated cabinets over treated ones.

9/3/13       #8: Bora Care causes glue adhesion issu ...
mark

The answer is, no, but I'll at least guess: Bora care is formulated for stick-built houses to treat the framing. Framing lumber is 12% to 15% MC. Borates are readily water soluble, and I assume that this is the way that Bora care migrates into wood. Your cabinet material is 5% to 7% MC, so there is not enough water present to allow the treatment to migrate away from the surface. Then you glue with titebond and voila, there is water! So, your Bora care residue permeates the glue and makes it ineffective.
Solutions? Run this by the Bora care folks, and see what they have to offer. Treat lumber before drying. Add a little water to the Bora care to help it penetrate. Try a different glue, like Unibond, and see if you have the same issues when you're not adding water at the glue phase. Recalculate the amount of product that you spray on sheetgoods to reflect the fact that only the outer veneer is permeable.
Just some wildassguessing, but I figured it might be more helpful then telling you to move to Vermont.

9/3/13       #9: Bora Care causes glue adhesion issu ...
antonio

Mark, thanks!!! much things are said with few words,,, i REALLY appreciate that!! very useful info. Not sure if you have used the 'bora care' product itself before but seems like you know the principle behind it, as you said, it is just borates mixed with glycol (same as in antifreeze?) supposedly the glycol makes the borate penetrate the wood deeper. thing is , when i first mix the bora care 1:1 with water , that batch goes on very well with little 'salt' left on the surface ,, but seems like when i let this diluted batch sit for a few days that the salt doesnt seem as soluble as when i first mix it, ,,, if that makes sense,,, so when i apply that 'leftover batch' to wood, that stuff leaves the most salt behind after it dries. So yeah i guess i should be behind the manufacturers as to what i can do about this... Thanks again,,,,,and actually am thinking about a migration ,,, but to canada if i can find a good hookup to setup my shop up there :)

9/20/13       #10: Bora Care causes glue adhesion issu ...
correy smith

Great answer mark. I might add here in Hawaii, it is common just to gas treat the finished product in the same manner you would your house. After your canibets are complete prior to delivery, you have the local pest control come by on Fri afternoon. They drop a big tarp over the job and gas it. It sits till Monday you install that day if you like.
You need to throw out all the heavily infested pieces. Treat what is salvagable. I routinely gas treat loads of lumber I buy. I take my trailor right to the Bug guys and thay tent my trailor I pick-up the next day. Like $30 for 500bft-ish.
YOu should be seeing obvious entry holes and the such as your culling pieces for your job. Are you intentionally using wood that has obvious holes in it?
It's exceptionally hard if your in an area heavily affected by termites not to have them in your shop. Swarming season and they are coming in no matter what. Best to have your shop tented periodically. If they were present prior to your leasing maybe try and split the cost with the owner of the structure.
I wouldn't spray finished material with any thing. Bugs should be held off with treated or other preventative measures until processing. Then the final gassing if need be.
I found the gas treatment to be 100% effective in 8/4.

2/15/14       #11: Bora Care causes glue adhesion issu ...
Gene Wengert-WoodDoc

BoraCare is put into the wood using water as the carrier. After application, the water moves to the surface where it is evaporated. This leaves a concentration of the chemical at the surface (like the ring left if you evaporate the water from a dish a salt water). Before gluing if you remove this outer surface by very light sanding, you will be in fine shape for a strong glue joint. However, if you sand and then the wood dries a bit, you will likely not be as good; so, sand just before gluing and remove the dust.

One question is if the BoraCare dust is safe to breath or do you need to take special precautions.

10/14/15       #13: Bora Care causes glue adhesion issu ...
JP

I wish my cabinet maker has done it.
My new natural wood walk-in closet is now infested with termites.

10/15/15       #14: Bora Care causes glue adhesion issu ...
Gene Wengert-WoodDoc

JP,
Where are you located? In almost all of the US termite zone, we are dealing with the subterranean termite. This insect needs a connection with damp soil and makes tunnels between the water supply and the wood. These termites do not like dry wood. So, to have termites in cabinetry in a closet is extremely rare. The treatment for existing infestations is usually accomplished by treating the soil, and/or their entry way, and not the wood. Avoiding high moisture levels in the wood also helps with termites, as they do not like dry wood. I would also guess that damp wood for closet cabinets would be undesirable...dry wood would help keep clothes better and more free of mildew odors and the like.

Also, if there are termites in your cabinets, it is likely that they are in the framing of your structure as well as (OSB or plywood) wall or roof sheathing (seldom are these products treated for termites prior to installation) and other untreated wood, so you have more of problem than just cabinets.

There is another termite that does not require this water connection, but flies to water...this is found in the USA in FL, and along the Gulf Coasr sometimes, as it needs warmth and humidity.

1/24/21       #15: Bora Care causes glue adhesion issu ...
Linea Speer Member

We milled about 650 bd ft of an oak and the ppb were pretty bad. After using bora care I noticed the same glue adhesions issues. If I plane the wood it glues up fine. Usually 1/32 off and the glue functions well.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!