Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Endgrain Inlay

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Endgrain Inlay

2/18/21       
Kris Member

Hi all,

Having a problem with a vanity top.
The designer is asking for an end grain oak inlay to make it look like the wooden vanity top has four wooden legs holding it up with through tenons.

The rest of the top is oak veneer on marine ply.
The size of the inlay is 3.5x3" square, 1/4" thick.

On the sample top, the inlay started cracking and warping up.

It was only finished on the top, so do you guys think that sealing on all sides before install would prevent that the warping? would going 1/2" prevent it? 3/4"?
Do you think it's an issue of warping up, or expansion and contraction issues?

We would prefer not doing an end grain inlay on a vanity top, but that isn't an option unfortunately.


View higher quality, full size image (5760 X 4312)


View higher quality, full size image (5760 X 4312)


View higher quality, full size image (5760 X 4312)

2/18/21       #3: Endgrain Inlay ...
duster

It looks like your solid oak end grain inlay shrunk and then cracked, most likely because it wasn't dry enough. Making them thicker won't solve the problem. I'd try making them thinner and make sure they're dry. Also, maybe try epoxy instead of a water based glue, which may add moisture to a porous end grain inlay.

2/18/21       #4: Endgrain Inlay ...
TonyF

Kris:

Way too thick. What you might try is to cut the end grain as you did before but 1/8" thick and epoxy it to a piece of 1/4" Baltic birch ply, with a veneer backer as balance, and then run it all through a widebelt sander with the end grain up until the end grain is close to veneer thickness, and then inlay that into your veneered top. Use a waterproof glue to adhere the inlay into the top.

Designers!!!!! (screamed like Capt. Kirk screaming Khan!!!!!!)

Good luck.
TonyF

2/18/21       #5: Endgrain Inlay ...
rich c

You've never heard of seasonal wood movement? Buy Bruce Hoadley's book, Understanding Wood.

Understanding Wood

2/19/21       #6: Endgrain Inlay ...
Mark B Member

My approach would be to super dry your endgrain inlay (heat, toaster oven, low oven, however you can), leave it as thick as you wish (within reason but a bit thicker wouldnt be bad) because the conventional rules of wood movement as it pertains to veneer dont apply here, and run your inlay with either PVA or Epoxy as normal. Super drying the inlay will mean that the instant it comes out of the heat it will begin to take-on moisture an expand. It will be somewhat like inlaying a compressed dry sponge and as it takes on moisture it will expand into the cavity. This will keep the inlay in constant compression likely holding throughout seasonal movement for eternity.

Being end grain and relatively small the expansion will have zero effect on the top but the small inlay will be forever trying to expand having the best chance of keeping the joints tight.

My approach would be to leave the inlay relatively thick and take it down to the surface with a flushing router jig/lamello lipping planer/whatever you have. At least that way the inlay will stay as flat as possible and allow you to clamp it in place.

Concern with running the end grain inlay very thin would be whatever glue/epoxy you have coming through the capillaries even with non-white oak species.

Just my $0.02

2/19/21       #7: Endgrain Inlay ...
Kris Member

Thanks very much for the responses!
Some great ideas to try out

Really appreciate the help

2/19/21       #8: Endgrain Inlay ...
Tom Gardiner

I see two issues here. One, the shrinkage and cracks and two, poor glue adhesion.
Both can be addressed with an epoxy joint with the caveat that the epoxy will wick up the open cells. Can a filler be added to the epoxy to increase the viscosity?
Last note. Is that a water borne finish? If so it likely contributed to the failure because the end grain would have been an open avenue to the pva glue bond further weakening it.

2/19/21       #9: Endgrain Inlay ...
Kris Member

Thanks Tom

It is a 2k polyurethane finish, and a pva glue.

To be honest, I've never used an epoxy to glue before, but I'm game to try.

2/19/21       #10: Endgrain Inlay ...
Mark B Member

Over dry your inlay and walk away. If the endgrain inlay is going to move, shrink, cup, your dead. Come as close as you can to eliminating those and walk away.

We have a good customer that spends with wreckless abandon but for whatever reason buys a good bit of furniture from sh(tholes like Ashleys and Wells. Tables with this same faux element have gaps that will hold a half a teaspoon of cheesy goop that falls off someones fork. Its accepted, and dealt with.

The over-dry inlay will get you closer to something you can sleep with though likely not perfect. Your finish has zero to do with your problems.

Welcome to 2021

2/19/21       #11: Endgrain Inlay ...
Dave Sochar Member

At the risk of sounding like a jerk, how is it that you come to do work you do not know how to execute?

I do not mean to call you ignorant or incapable, but these are fundamental properties of wood you can ignore with box work or such. But when you get away from boxes (or whatever is your daily bread), beware. You need to know what you are doing. There might be a reason you have not seen this before.

Was there no one in the shop that raised a hand with this problem? Some wise guy that was being negative and not getting behind whomever's solution this was?

2/19/21       #12: Endgrain Inlay ...
Kris Member

Hi Dave

The full(ish) story is that this is actually a project we were brought into late in the process.
The job was originally meant to be produced in China, but for a number of reasons they decided to bring the project back here, and asked us to step in after design decisions and samples had been made and approved.

The sample above is the one produced by china that was shipped here.

We red flagged the endgrain immediately, but the samples had been approved so we were told to match the construction method here.
The pictures above are actually from the sample from china, we haven't done our version yet, because after a few days in the shop, the inlays did this.

I didn't want to overwhelm the forum with useless details that wouldn't help resolve the issue.

I really appreciate all of the ideas on this.
And I definitely agree, there is a reason we haven't seen this before, and I plan on not seeing it again after this job.

2/20/21       #13: Endgrain Inlay ...
Mark B Member

Sounds like a pretty decent opportunity. They clearly got what they paid for. Its crazy the stuff you see when you walk into a bread and butter furniture store now. The things the public are wanting/accepting are completely nuts. But the pricing, when you add in the retail margin, there is no way to be competitive. Good luck, nice to hear about a chance for something to come back.

2/21/21       #14: Endgrain Inlay ...
Dave Sochar Member

You have to love failure. It is a great way to see what doesn't work. Especially when it is someone else's failure. Not to wish bad on anyone, but their problem helps our/your solution.
This now makes sense, and you have some good ideas that should make this work. I am of the 3 ply veneer - end grain faces on a straight grain center - camp.

Please post what you end up doing and how you did it. It is the process that is interesting.

2/22/21       #15: Endgrain Inlay ...
TonyF

Kris:

Epoxy absorption can be an issue on end grain. What you might try is the West System 105 resin, whatever of their hardeners suits your open time requirements, and their 406 Colloidal Silica as a thickener.

Sounds like it might have been easier to just actually mortise a leg through the top.

Good luck.
TonyF

2/23/21       #16: Endgrain Inlay ...
Mark B Member

Dont really understand the distain. You have a client that can potentially feed you with decent repetitive work and you can either be a problem solver or a problem finder. Opting to solids and true mortise exposed thru tenon is a guaranteed failure on price and product.

Sucks that as materials advance the boundaries of tradition get pushed (and often pushed too far) but the answer is your business will rely on those connections.

I find the option of a faux tennon disgusting but when push comes to shove and you have an application where it could fly, and you can get paid,.. it is what it is.

We are never going to stomp our feed and dig in our heels and force the country into boutique. Its just not gonna happen.

So you adapt or die. Or get a job somewhere.

2/23/21       #17: Endgrain Inlay ...
TonyF

Mark B:

My through mortise comment was more tongue-in-cheek, rather than to be taken literally, or to put forth any disdain for those who allow us the opportunity to work on something more challenging than Motel 6 vanity tops.

I did offer up a method that I would use to accomplish the task in question, and that Kris might consider, rather than to endlessly bitch about designers and their designs.

I know that myself, and probably everyone on this forum, has met with a similar circumstance to the one that Kris has, perhaps even on an ongoing basis.

Please don't confuse the verbal hooliganism about designers with disdain, as at one time I worked exclusively for designers, and more than appreciated some of the interesting work that they threw my way, as well as the paycheck that would accompany it.

I also occasionally complain about my wife, but it is more minor venting about the little things that piss me off, rather than having contempt for the finest human being that I know.

Intent and context is everything. Sorry if you misunderstood.
TonyF

2/24/21       #18: Endgrain Inlay ...
Mark B Member

No issue with regards to my response was directed any anything/anyone in particular Tony. I think any of us would take the route of a through tenon by default and likely advise the client, though it does have issues of its own with the largest one unfortunately being cost which is clearly why the faux veneer top is on the table.

I wasnt in any way intimating with regards any response. Just moreso that as sucky as it is, this is a situation where the spec'd solution would likely fly just fine with todays consumer with some good practice and get the job paid. The failure in the images seems to be solidly a manufacturing issue (poor practice, pieced end grain inlay, and likely a pretty wet ride back to the states in a container load) not an issue of a 3.5" square end-grain plug in a veneer sheet being a guaranteed failure. After all even the shrinkulator calls out 3.5" red oak with a 5% swing at .003-.006 to the larger.

Apologies if you thought I was referring to your through tenon directly.

2/25/21       #19: Endgrain Inlay ...
Kris Member

Well, some very good news, and maybe slightly dissapointing news for you guys.

Very good news, we talked the client into removing the end caps on this project, which will let us sleep a bit easier for sure.

Unfortunately I probably won't through sampling these different options for quite some time.
I'm interested now, so I'm going to try to do some testing to see what happens, but that's pretty low priority at this point.

I will post my results when I get them for whoever is interested.

Thanks for all the help though.
I really appreciate the advice you guys are consistently able to deliver.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!