Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Chair construction, for "large people"

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Chair construction, for "large people"

4/3/15       
Cleabane

So My wife is a big girl. After a few kids, she weighs in at 330 lbs.

I want to make her a chair, for her 35th birthday.

Obviously the design considerations differ, a bit from chairs we would build for smaller individuals. Really not sure how to test these sorts of things, since I weigh about 165 lbs myself.

Considerations are totally different. Concerned that even stout mortise and tenon joinery, might not hold up to well long term.

Anyone have experience building chairs for larger people?

4/5/15       #2: Chair construction, for "large ...
D Brown

Maybe select a Mission or Stickley style
chair to build and beef up the frame members if need be .Good luck .

4/5/15       #3: Chair construction, for "large ...
Cleabane

That would be nice. the chair is going to be used for the weekly bible studies she hosts.

4/6/15       #4: Chair construction, for "large ...
Walt Turpening

Website: https://www.facebook.com/WTBSC

I make woven seat style seating. The seat rails are 1" to 1 1/4" hard maple dowels depending on the span. I use 1 3/4" to 2" leg and back stock. 1" deep 1" round mortise and tenon joinery.

I have made chairs for 'large' people. Up to 375# and 6'8". I have a rocker I made for myself (290#, 6') 17 years ago that is my daily 'user'.

I have only had one part fail on a large Settle and that was not the joinery. The 1" hard maple dowel side rail had a green stick crack. The way the seat is woven prevented full failure. The Settle was repaired and now 15 years later still in use.

Take a look at my pieces on the web page. Photos go to Albums and then Rockers.


View higher quality, full size image (2310 X 2805)

4/6/15       #5: Chair construction, for "large ...
D Brown

Walt , that is a beautiful chair and I love the pattern you wove , well done .

4/6/15       #6: Chair construction, for "large ...
markbattles Member

Website: http://v-dubfurniture.com

Hard maple dowel side rail had a green stick crack. The way the seat is woven prevented full failure.

4/7/15       #7: Chair construction, for "large ...
Walt Turpening

Website: https://www.facebook.com/WTBSC

One of the 'dynamics' you need to consider is how a person gets out of and into their chair. The seat height needs to be tall enough for them to stand up not have to 'climb' out. The worst furniture is that soft 'crap' that you sink down into. Make the seat firm enough but still flexible for comfort.

Second, make the seat to fit their seat depth, back of knee to their back. I typically make the seats 2 inches less than the measured length on the person.

Make the chair for your wife and only as a secondary point consider some particular 'style'. Since it is for her to teach, do not make the back more than 15 degrees angle to the seat. Make the front edge rounded to minimize pressure on the backs of her legs. Soft padded edges are not the solution.

4/7/15       #8: Chair construction, for "large ...
B.H. Davis  Member

Website: http://www.curvedmouldings.com

The failure point in the typical chair is where the stretchers meet the flared legs. For a chair like this I would avoid flared legs unless they are captured at the bottoms similarly to on a rocker.

BH Davis

4/7/15       #9: Chair construction, for "large ...
Walt Turpening

I agree with B. H. Davis. I use pegged M-T's on the stretchers of all my pieces. In the design process, I had the stretchers pull out during the weaving process or shortly after a piece was done and in use.

4/8/15       #10: Chair construction, for "large ...
Roscoe

I would build it to hold between 500 and 600 pounds. Plan for what the future holds.

4/12/15       #11: Chair construction, for "large ...
Jeff H Member

I built the straight arm morris chair for myself. I'm a pretty big boy and the chair is rock solid. Fairly large mortise and tenons were use. I'm a wide fellow also and I have room in this chair.

10/3/21       #12: Chair construction, for "large ...
Frank McGuire Member

There are a lot of manuals and how-to guides on youtube on how to build it. To my mind, isn't it better to pay attention to ready-made solutions on the market?

https://www.reclinerland.com/best-recliners-for-sleeping/

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!