Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Material or treatment advice for outdoor furniture??

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Material or treatment advice for outdoor furniture??

4/5/21       
Ringwall Member

I have recently been commissioned to build a hundred plus units of children's picnic tables and sandboxes. I am not a professional woodworker, but an advanced DIY'r in an MBA program, with a background in manufacturing management.

I am partnered with an experienced contractor, who is a capable builder, but not specifically a woodworker. I was hoping to get some advice on here to aid me in making some informed decisions.

I built the prototype out of cedar for the customer, as they are a higher-end retailer, but they want to keep the costs down for seasonal goods. The mill where I purchased my lumber also said that cedar was less readily available (at least right now) and they recommended pine, which they had heaps of, it was more affordable and more regular in shape.

I do not have a lot of experience building for outdoor use, aside from fixing up my old deck. My understanding (and pardon my naivety) is that the most common woods for this type of application was cedar or pressure treated wood (Lowe's calls it pressure treated wood, and does not indicate what type of wood it actually is, during my cursory research)

The pine they had at the mill did not appear to be treated at all, and in a best case scenario I would prefer not to use pressure treated as it seems to be expensive and often unavailable in Ontario these days, and furthermore, less attractive for kids to be playing with.

So all that being said, can I use pine to build these tables and then seal/stain/paint them to protect against the elements, or must the wood be pressure treated? If this is an option, what seal/stain/paint would you all recommend?

Other than cedar, is there any wood you would recommend that is robust enough for the outdoors, but affordable enough to be practical?

This is my first post on woodweb, and I was warned that you guys can be tough, so I'm wearing my thickest skin in preparation for your answers ;)
Thanks in advance.

4/5/21       #3: Material or treatment advice for ou ...
duster

I would avoid using pressure treated material for any furniture or playground equipment. The chemicals used to resist rot and insects are also toxic to humans and animals. Pressure treated wood can also be kind of splintery, which is also good reason to not use it for kid's furniture.

Cedar or redwood would be your best choices if the budget allows for it. Pine is ok, but won't last as long in an outdoor environment. If you're going to put a finish on it, I'd use an exterior deck stain instead of paint.

4/6/21       #4: Material or treatment advice for ou ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Greetings,

Redwood and cedar are expensive indeed. Also, redwood has been on a protected species list for many years and likely would be difficult to locate in the quantities you describe without special license.

For kids tables and sand boxes that will last a lifetime I would look into the composite products similar to “Trex”. It machines similar to wood, looks like wood, does not splinter, holds screws well and will last into the next century. All of your big box lumber yards will have it in stock. It is also sized like wood....1x4, 1x6, etc...

I’m not sure about the cost.

I never realized pressure treated wood could be so hazardous chemically. It is literally all around us. Decks, bridges, picnic tables, sand boxes and more. Pressure treat wood is always southern yellow pine.

Dennis

4/6/21       #5: Material or treatment advice for ou ...
Dave Sochar Member

Without an experienced woodworker, preferably a chairmaker, or furnituremaker at the least, your project is doomed.

DIY, MBA, experienced contractor all add up to something less than zero.

As a professional woodworker with over 50 years experience, I would like to take a job that normally requires an MBA. I mean, how hard can it be? What I do a on a daily basis is simple and easy. So easy, anyone could do it. No training or knowledge required.

Why is it that people from all walks of life think they can be a professional woodworker based upon their desire alone?

With building 100 units of children's furniture - who will carry the liability? Have you investigated what that liability coverage will be? If not, double the price for each item.

Species? You are just starting to get into that one, and already you are being steered away from wood (note the person doing so is not a woodworker). Joinery? How big a screw can your drill drive? Mortise, tenon, aren't they all things of the distant past? Design? Can the pieces be repaired easily? Can they be easily procured from sustainable forest products? How about finish? Toxicity? Renewability?

A tough crowd? Or realistic and a little insulted?

4/6/21       #6: Material or treatment advice for ou ...
Glen Harwell

We have been building custom furniture for forty years. We never take on any work involving children's furniture. No cribs, no toys, no sand boxes and no picnic tables. There is a huge liability risk. I would never use pine outdoors. Cheap for a reason. We build custom patio furniture using teak and mahogany. Good luck.

4/6/21       #7: Material or treatment advice for ou ...
rich c

Modern redwood is crap. If it has sapwood on it, it won't last 3 years. They still sell it on the reputation of old growth redwood, it's like 2 different woods. Cedar can be horrible for splinters. Nothing you want for children's furniture. Speaking of children's furniture, you will need a ton of liability insurance. I mean a multi-million dollar policy. Just ask IKEA what it cost them for kids chest of drawers tipping over. Same goes for your picnic table if the kid falls over backwards if the table tips a little. Why is it up to you to fit their price point? Let them spec the material or you will be liable for rot, splinters, peeling finish, etc....

4/7/21       #8: Material or treatment advice for ou ...
Cbww

Anything for a child I walk away from. Bunk beds/cribs...just not worth it. Plus they are basically all throw away pieces. Same goes for anything outdoor. Pine will rot in a few years. I made some outdoor chairs for myself with my son- his school project- but it was white oak, mortise and tenon, epoxy. I actually grooved the tenons/mortise slightly to create little ridges to hopefully lock the joint. Seems like it worked. No finish will last outdoors for very long unless its maintained regularly. Your job sounds like a headache and I wouldnt waste time on it.

4/8/21       #9: Material or treatment advice for ou ...
Thomas M Diel  Member

Website: http://thomasdiel.com

Not to beat a dead horse but really?

If you don't have liability insurance you better look into it before you sign or receive payment for a production run. Your designing and fabricating ie your shouldering all burden (strict liability) - your screwed. My insurance is my second biggest fixed cost behind rent and I can't go anywhere near children's furniture; but I have done many other life safety issues that are issued certs for - always with architects stamps behind them. But kid stuff in the public sector, wow, wow! Even a tight, one year limited warrantee won't protect you in this realm.

A big second thought is are you protected under any corporate umbrella or sole prop?

But to get to your question: White oak on the wood; maybe osage orange (bodark), mesquite, teak, but nothing soft, it might last a year. You might find some imported rubber wood, but I have never worked with it? My designers degree & 30yrs of makers two cents worth.

4/11/21       #10: Material or treatment advice for ou ...
duster

Wow. I never knew there were so many guys scared of making furniture. The bulk of my 38 year career has been custom residential furniture. Millions of dollars worth.

Tables, chairs, beds, dressers, desks, armoires, TV & stereo cabinets. Hundreds of bunk beds, an entire product line of childrens furniture. Picnic tables, benches, barstools. A bunch of weird, one off pieces that interior designers dreamed up.

I build stuff to the best of my ability, being careful to engineer pieces so they don't fall apart. No one has ever tried to sue me. I do have liability insurance, but I've never needed it. If clients are adamant about a design I'm not comfortable with, I turn it down.

I'm not scared to try new things just because someone else got sued. I just make sure quality is built into my pieces. Then I cash the checks...

4/12/21       #11: Material or treatment advice for ou ...
Glen Harwell

We have made 40 million dollars worth of residential furniture. We have never been sued either and I want to keep it that way. We just stay away from baby furniture. We do plenty of beds, dressers and night stands just no play furniture or cribs. We will leave that market to you.

5/10/21       #12: Material or treatment advice for ou ...
Adam

Based on your lack of experience you need to carefully evaluate the risk vs benefit ratio in this proposed undertaking. It's hard to make money on furniture in general.

You want to build outdoor furniture. Expensive materials: rot resistant wood, epoxy, and only stainless fasteners.

Most people lose money on the first big project that they take on. Those people generally have reasonable experience building those things. Breaking even is considered a success.

I would be concerned about the quantity. You could lose badly upfront misestimating(no experience) the true cost of each unit. There is also the backend cost of warranty work. If you make a minor math error or they prove to be defective you could lose bigtime x 100.

Sandboxes are generally made out of plastic. Permanent ground contact would be treated. Even cedar would be sketchy.

I would look into red meranti for the picnic tables. It's a fantastic material to work. Beautiful. It's easily available in the North East. They use it primarily for decks. They have all of the typical sizes. 1x4-10, 2x4-6, 4x4.

I still have a red meranti furniture grade picnic table I built 20 years ago. It's sat fully exposed on our lawn, completely neglected. I sealed the end grain feet with epoxy. That's it. Rain, snow, sun. Weathers beautifully.

The liability the other guys have mentioned is real. You occasionally read about some crib or playground hurting some kid. You should speak with your Insurance broker about coverage.

If I were you I would sub it out. You are a business guy. Stick to being a middle man. It's hard to loose your shirt.

8/17/23       #14: Material or treatment advice for ou ...
FerdinandKola Member

Website: https://www.gardenfurniture.co.uk

I understand that the thread is a few years old, but the information shared here remains valuable for anyone else who might come across it while seeking advice on outdoor furniture. Your inquiry about material choices and treatments demonstrates your thoughtful approach to your project.
For outdoor furniture, using pine with proper treatment is still a viable option. Applying a quality outdoor sealant, staining, or painting can effectively protect pine against the elements. If you're looking for current recommendations and products, you might want to click here for updated information on sealants and finishes that can enhance durability

5/8/26       #16: Material or treatment advice for ou ...
Zavin Clark Member

Teak gets all the glory, but half the people who buy it forget it still needs yearly treatment. All-weather doesn't mean zero effort.
Honestly the best material is whichever one matches your actual lifestyle — not your ideal lifestyle. If you know you won't cover it, oil it, or store it in winter... aluminum exists for a reason.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!