Ideal temperature / humidity for solid timber furniture

6/5/22       
Nicholas

Hello fellow makers,

I've experienced some cupping on my solid American Oak tables in QLD and NSW recently, and I know they have been experiencing some unprecedented fluctuations in both humidity and temperature as of late.

If anyone has experience in this area, or knows some great resources
regarding standards for ideal relative humidity and temperature for furniture maintenance in the home, any recommendations would be greatly appreciated.

Regards,

6/6/22       #2: Ideal temperature / humidity for so ...
RichC

QLD and NSW? Cupping is either caused by not allowing seasonal wood movement, or moisture changes in the wood. Are you checking the moisture content of the wood when you buy it? Do you finish the bottom surface of the table like the top? How wide of boards are you using? Are you fastening a breadboard end rigidity to the table top? Lots more data needed!

6/27/22       #3: Ideal temperature / humidity for so ...
Dave Sochar Member

Queensland and New South Wales are my guess for the abbreviations. That is the other side of where you are Rich.
The US indicates that 35% RH is ideal for kiln dried woods in the 7 - 9% range. The Europeans favor it a bit more humid at %40.
Rich's questions are all valid.
Bruce Hoadley's book "Understanding Wood" is a good place to get answers.

9/16/22       #4: Ideal temperature / humidity for so ...
Kevin Jenness

Ideally work will be built with wood that is in equilibrium with the shop environment and its conditions in use. That will depend to some degree on local conditions. If the lumber's moisture content is more than a few points away from use conditions problems may ensue. When the wood is acclimated to the shop and construction and finish details allow expansion/contraction within projected norms issues will be minimized. As David S. said, Hoadley's book is a great place to start.

8/12/23       #6: Ideal temperature / humidity for so ...
Laura Member

Cupping in solid oak tables can indeed be a result of fluctuations in humidity and temperature. Wood is sensitive to changes in its environment, and when the moisture content of the wood changes, it can lead to issues like cupping, warping, and cracking. Here are some recommendations and resources to help you address and prevent such issues:

1. **Maintain Stable Environment:**

- Keep the indoor humidity levels as stable as possible. Fluctuations can cause wood to expand and contract, leading to issues.

- Use air conditioning or a dehumidifier to control humidity during humid periods.

- Avoid placing your furniture near heat sources like radiators or direct sunlight, as they can cause localized drying and warping.

2. **Ideal Humidity Range:**

- The general consensus for indoor humidity to prevent wood issues is around 40-50% relative humidity.

- You can use a hygrometer to monitor humidity levels in your home and make adjustments as needed.

3. **Temperature Considerations:**

- While temperature fluctuations can contribute to humidity changes, keeping the temperature relatively stable is also important for preventing wood issues.

4. **Furniture Placement:**

- Avoid placing your furniture in areas with extreme temperature variations, such as near doors or windows that are frequently opened.

5. **Wood Care:**

- Use a quality wood conditioner or furniture polish to maintain the wood's moisture content and protect it from drying out.

6. **Resources for Further Reading:**

- The Forest Products Laboratory (FPL) of the USDA Forest Service offers a guide called "Wood Handbook: Wood as an Engineering Material," which provides comprehensive information about wood properties, including its response to humidity and temperature changes.

- The National Wood Flooring Association (NWFA) also provides resources on maintaining wood floors, which can be relevant for furniture care as well.

- The American Institute for Conservation of Historic and Artistic Works (AIC) has publications on preventive conservation for wood artifacts, which can offer insights into maintaining wooden furniture.

Remember that wood is a natural material and will always have some degree of response to its environment. It's important to strike a balance between maintaining the aesthetic and structural integrity of your furniture while considering the realities of your specific climate and home conditions. If the cupping is significant and you're concerned about your tables, it might also be a good idea to consult with a local woodworking professional or furniture restorer who is familiar with your region's climate challenges and can offer tailored advice.

10/16/23       #7: Ideal temperature / humidity for so ...
Sara lopez Member

Website: https://holapaints.com/spray-painting-temperature/

Ideal Conditions: For solid wood furniture, including oak, the ideal relative humidity (RH) is around 40-60%, and the spray painting temperature should be maintained between 60-75°F (15-24°C). Use a digital hygrometer to monitor RH.
Humidity Control: Use a dehumidifier in humid conditions and a humidifier in dry conditions to maintain stable RH. This can help prevent wood from expanding or contracting excessively.
Avoid Direct Sunlight: Direct sunlight can cause rapid temperature changes and fading. Use curtains or blinds to protect your furniture from prolonged sun exposure.
Climatic Fluctuations: In regions with extreme climate changes, consider using a humidistat to control humidity levels. Seal doors and windows properly to minimize temperature fluctuations.
Regular Maintenance: Keep your furniture clean and use wood-specific polishes or conditioners. This helps protect the wood and maintain its appearance.
Helpful Resources: The Holapaints and Woodwork Institute the National Wood Flooring Association provide resources and standards related to wood and environmental conditions.
https://holapaints.com/spray-painting-temperature/
Consult a Professional: If you're unsure about the specific needs of your furniture, it's a good idea to consult a professional woodworker or a furniture specialist.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!