Subject: Re: Small gap at between Face Frames

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Small gap at between Face Frames

3/8/13       
Mark C  Member

My company is doing it's first cabinet install using a manufactured cabinet. There is a 1/64" gap between the Face Frames in some spots.

My carpenter says the Face Frames weren't quite straight and we need to use matching putty and fill the small gaps.

After thinking about this situation, I have a theory. I am hoping someone has some experience in this area.

We used Pony clamps to fasten the cabinets. The first time he used them he split the frame and said that the Pony clamps put the hole too close to the edge and that was the reason for the split. He started using the clamps for alignment only and hand drilled the pilot holes away from the clamp.

My thought is that there is a small gap because he isn't drilling right where the clamp is putting it's pressure. Then the threads of the screw are actually holding the two pieces apart?

I know putty must be used in some cases, but I would like to avoid using it on the Face Frames if possible.

Any help on this matter is greatly appreciated.

Mark C

3/8/13       #2: Small gap at between Face Frames ...
JeffD

Sounds to me like your problem is the installer. When everything else is causing problems that usually means the guy doing it doesn't know how to do it properly.

For instance, faceframes aren't perfectly straight? Break out a block plane and one or two swipes has them straight! You should need clamps only for pulling and holding the 2 cabinets together, NOT to straighten the faceframes! If your trying to force the faceframes straight by clamping and screwing I think putty is the least of your problems! And there has got to be more than a 1/64" gap as you could close that just by hand pressure? Hard to advise any better than that without actually seeing the problem, but it sure sounds like the installer to me.

good luck,
JeffD

3/8/13       #3: Small gap at between Face Frames ...
Gerry

Often when you pilot a hole when two pieces are being held together you get swarf between the two pieces when the bit comes through the first piece this will hold the two pieces apart if not cleaned out. Another problem is if your pilot is not over sized in the first piece and you screw is threaded all the way up it will not pull the two pieces together.
A installer who is not aware of these problem either doesn't have enough experience or doesn't care.

Gerry

3/8/13       #4: Small gap at between Face Frames ...
Jerry Fartwell

Get a new installer. Don't putty the face frames. Pull out the screws and fix the problem.

3/9/13       #5: Small gap at between Face Frames ...
mastercabman

I also think that the installer is the part of the problem.
Those pony clamps you use,Are they the
"face frame pony clamp"? If so,i got a pair of them and used them for about 2 weeks,that was years ago.I use kwikclamp made by BESSEY and use a 4mm bit to drill my holes.I also use 2.5" square drive screws to attach cabinets to each other.

3/9/13       #6: Small gap at between Face Frames ...
mark

Some good ideas here, but they all seem to be affected by the op's pawning off of responsibility.
Mark C., your description of the situation suggests that you don't have much experience with cabinet installation, and that you're trying to get out of paying for skilled and knowledgeable help. I could be misreading the situation, but this is what I think:
1. Filler is for under finishes in places where there is no possibility of unevenness in the movement of the surrounding material.
2. Clamps are not fasteners, clamps are not drills, clamps are not cabinetmakers.
3. Your carpenter would likely be put to better use on other tasks.
4. If you don't know how to drill a pilot hole and put in a fastener, then you should hire someone that does.

3/9/13       #7: Small gap at between Face Frames ...
Robert

I guess when I read manufactured cabinet...I think cheap and to be honest 1/64th on a cheap cabinet, well I think you got off easy. All these guys are giving you great tips for someone spending money, but if this is "cheap" then 1 /64th is nothing, less than nothing and when the tops are on and no sunlight coming through you'll be fine.

Some guys on here forget you get what you pay for. If you are hiring a guy at $30-$40 bucks a box be happy you aren't seeing 1/16th+ gaps.

Just my two cents....

3/14/13       #8: Small gap at between Face Frames ...
Jeff M

If your screws are pulling tight with no debris between the frames and you still have a gap, that's a good sign that your frames aren't straight enough. As mentioned above, straighten them out after some trial fitting. You should be able to pull two stiles together tight with just a couple of quick grip clamps and a couple of screws. Make sure your counterbore is deep enough so the screw thread will catch enough meat of the wood not to strip out.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)