Laminating and Solid Surfacing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Solid surface tops.

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Solid surface tops.

6/20/21       
Scott

I have never worked with solid surface countertops before, I am building a front counter with a solid surface top.
I have done a lot of research and read a bunch of posts and watched a bunch of videos.
My question I guess is there much of a difference between material? I was planning on using Wilsonart material as I deal with them for other stuff. I worked with plastic laminate for years and we always tried to color match on solid colours because our shop preferred Wilson art or Formica, I am curious if there is a preference for solid surface ?
Thanks

6/23/21       #2: Solid surface tops. ...
Bruce H

It's not difficult to work with, results will vary depending on how well you follow the rules. Usually it requires certification to purchase material, you might get someone to sell it to you. Not being a certified fabricator what you won't get is any kind of warranty. You can easily get certified, find a supplier that has classes and sign up.

The difference between brands is mostly color and patterns. The chemical composition is about the same as are working requirements.

6/23/21       #3: Solid surface tops. ...
Bruce

Bruce,
Thanks for the information, I am not a fly by night guy, actually more of a perfectionist, I just thought the course and training was only a corian brand thing.
I will ask the wholesaler about taking a course.
Thanks again.

6/29/21       #4: Solid surface tops. ...
Mark B

I think what you'll find with most of the off-brands is there really is no training. Depending on your location and who else is fabricating in your area you may or may not be able to even buy some brands. If some of the bigger brands have a single or a few fabricators in your area you likely wont even have access to purchase (wilsonart, corian, etc.). In our area Formica, 909, Livingstone, LG, Durasein, Aristech, on down the line, are pretty much wide open. Their "training" will be a PDF/video.

Even with the big boys the warranty is not necessarily a material warranty as your likely never going have a material failure. The training is there so you represent the product/brand suitably. Most any failure your going to have will be a fabrication flaw and that will be on you period, not the product warranty.

7/2/21       #5: Solid surface tops. ...
Scott

MarkB,
Start off by saying I replied to Bruce and put my name as Bruce as well, sorry about that.

I have only talked to two wholesalers, they said they would sell to me and like you said, they said there was not really a course, one was Wilsonart and the other Formica. They are the same wholesalers I buy all my materials from so it is quite convenient.
Apparently there is data on there website for working with the product.
Maybe I will find a supplier who offers a course and take it just so I am confident with supplying a professional job all around.

7/2/21       #6: Solid surface tops. ...
Bruce H

I got my training from Corian and Wilsonart. At the time they were real picky at whom fabricated the product. It was never rocket science, just plain common sense. I'd suppose with the changes in economy the classes offered got dropped. There is a lot of information online. Watch a few videos and you'll be go to go.

Tom Pinske (The Pinske Edge) has a great video he did with Dean at Hometime. Tooling ramp up on a one off top might be a little far out. I have over a dozen routers set up with bits ready to go. fifteen dozen clamps and the list goes on...

7/3/21       #7: Solid surface tops. ...
Mark B

I took the Corian course a long while back and it was clearly a course in protection of the product/brand which makes total sense. They dont want a bunch of yay-hoo's out there shipping "corian" tops (corian being a bit of a trade name for solid surface in general) that fall apart giving "the product" a bad wrap.

Wilsonart in my area (small) is not available to us because another shop is fabricating for the home centers and is very protective of that market. Corian has no distribution in our area without massive freight charges and their pricing of material prices them out of the market anyway. Formica, and all the others, are wide open. We do commercial work and if your the competitive bidder the architects will pick from your offering period. Its very rare, other than collusion or a match job, that a specific brand is the only option.

Bruce is spot on. Anyone is going to struggle to be competitive on-mass unless your setup. Swapping tooling between a hand full of routers, not having CNC, not having a way to deal with the colossal mess that IS solid surface, makes it a nightmare. In our small shop, were it not for the CNC and cutting everything and anything possible on the CNC, for the mess and cleanup alone, it would be a loser.

There is a local top shop here that I have no idea how OSHA has not cleaned their clocks. The place is like a snow storm. Chips and dust EVERYWHERE... fine powder from uncollected sanding and routing, guys walking around completely white in dust other than a mask and goggles. But they make miles of tops.

The granite top shop crackdown would seem to be headed squarely at any top shop that works with any of this.

7/5/21       #8: Solid surface tops. ...
Scott

Thanks for all the great info guys.

I was wondering what tooling you recommend, and what are your feed and speed recommendations for cutting on the cnc?

On a side note I was going to make a coffee counter with an L shape top, the top is 30 inches wide, so I have already bamboozled myself on making the inside corner as the material comes in 30 inch widths. According to the manufacturer you don’t want a seen there and the inside corner should have a radius. Back to the drawing board and learning curve.

7/5/21       #9: Solid surface tops. ...
Mark B

Reading through the fabrication info will give you all the information with regards to basic construction. Tooling is wide open and feeds/speeds are pretty machine dependant. Get in touch with the Mfr. rep in your area for the product your using. They will be far more help than anything you'd find here or online

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Today's Sponsors
    • Rose Machinery
      Horizontal Band Re-rips, Standard & Custom Designed Machinery
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • American Fabric Filter Co.
      Provider of Custom Made Filter Bags and Transfer Sleeves
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • WoodJobs.com Search Consultants
      Free Employment Service for Woodworking Related Job Seekers
    • Sandman Products
      Affordable Sanding Tables and Inspection Lighting
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Industrial CNC
      Affordable, Easy, Industrial Grade CNC Routers for Woodworking and Cabinetmaking - Free Lifetime Support
    • The Millwork Studio
      Millwork Shop Drawings and Estimates
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!