Bent wood laminations

1/2/20       
Chris Member

I'm a carpenter by trade and have a full-time woodworking shop that I do for my projects. Currently making a 36-in exterior door that has an 18-in radius top and I made a laminated door jamb out of four plies of poplar. Skipping ahead through the basics of a proper bending form I got approximately 5/8 of an inch spring back. It's approximately 70 in my shop I use tight bond three and placed my calls and clamps about every 5 in around the perimeter of my lamination. Any thoughts on how I can limit the spring back being as it is a door jamb the reveals have to be somewhat perfect any suggestions are welcome thank you.

1/2/20       #3: Bent wood laminations ...
Chris Member

Also to describe my form I did a full 18 in radius from side the side and to extend the jamb legs down I've got two 5inch
straight legs perpendicularr to what would be the bottom cord of the circle

1/2/20       #4: Bent wood laminations ...
David R Sochar Member

You will get better responses if you post this in the Architectural Woodworking Forum.

One thing you can be sure of, anything made of bent laminations, coming off a form, will not be what you planned for. Or needed.

There are formulas and rules of thumb, and other methods (dart board) - none of which are accurate except by chance. Generally, the more laminations, the closer the laminations are to what the form is. Four layers of Poplar will not hold much of a curve. You also need to use a rigid setting glue. TB III is the opposite of what type of glue you need. TB I, epoxy, resorcinol, urethane, plastic resin, will all work well.

However, I seek to change your ways. I suggest a 'brick laid core with a face". This gives you a sawn curve that is accurate and predictable. Saw out blanks to the inside radius, plus 3/32". Glue them together, to get your 6-5/8" or what is needed. Butt the ends of your blanks by cutting to a tangent. Once out of the clamps, clean up the inside face and add a 3/32" thick piece of Poplar or whatever to present a clean face.

If you are making a rabbeted solid jamb, then you will need to make two assemblies, one with a 1/2" longer radius than the other, to create the rabbet.

The sawn core is rigid and predictable. The thin face is pliable and glues easily, and presents a good look. No form needs to be built. Looks as good as bent laminations, but performs better.

1/6/20       #5: Bent wood laminations ...
bill Member

David I am not sure I am following what you are saying.

Do you have a drawing or photo that will help me visualize it?

1/6/20       #6: Bent wood laminations ...
David R Sochar Member

Bill - Let's say you need a 36" inside radius head - ISR. And being a door jamb, you need to end up at 4-5/8" wide, and 180 degrees.

Make a template - layout one curve at 36-1/8" and another, concentric at 37". Cut out and reproduce onto your wood - surfaced, flat and true. Let's say your wood is 1" thick. Lay your template and trace onto the wood so as to get as many parts out of the piece of wood as practical. Saw them out. Cut the ends so they can butt to each other when placed into the arch.

Draw your two radii onto the bench or plywood or where you plan to assemble. Lay your parts onto the drawn curve and build it up staggering the joints - bricklaid.

Take it down, spread your glue and rebuild. You can nail as you go, or clamp a couple of pieces, then wait and add a couple more.... Then you will have a curved wall, greater than 180 degrees, and 5" tall. Clean up with a sander and or scraper. Add a 1/8" solid ply to the face, using several bending wood cauls, and clamping every few inches. Use a rigid glue line glue for this last step. TBIII or equal will allow that skin to creep.

When completely dry, pass it under the planer, over the jointer, or thru the saw to get it to 4-5/8"

1/8/20       #7: Bent wood laminations ...
rich c.

2nd post on here where poplar and exterior doors have come up. Even for a jamb, poplar is horrible. You will get minimum spring back if you use thinner laminations and a glue that is rigid when cured. I can't say how much thinner of stock since we don't know what you used.

1/20/20       #8: Bent wood laminations ...
pat gilbert

The springback is greatly reduced if you use plastic resin glue.

2/25/20       #9: Bent wood laminations ...
dan summerhill Member

What we do is make a band saw swing table at 19R. Poplar is fine for this. Cut 18-24" long boards ( 4 or 5/4 work best) and band saw them each to get pieces not less than 1" at the ends. This gives you a stack or arcs, all with a 19R on both sides. Take the top offall from one board and clamp it to the bandsaw table square to the blade leaving 7/8 between the top of the blade and the inside of the arc. Slide all the arcs through the saw. you now have a stack of arcs 19 OSR ,18.125 ISR. We put a sled on the table saw and cut all the ends, again using the top of the first bandsaw cut as our cradle. You now stack these, glueing and stapleing as you go until you have built a jamb head. You either build to size or cut the ends when you're done. I like to cut at the end because it gives a perfect edge. Beltsand the interior and wrap it with 1/8 solid skin. You have a head that is 18ISR 19OSR. We do a 1" leg and shoot a scab on the outside.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Today's Sponsors
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Impact Search and Placement
      Professional Employment Recruiting Specialists
    • The Millwork Studio
      Millwork Shop Drawings and Estimates
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • ETK International
      New and Used Woodworking Machinery, Spare Parts and Superior Service
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Cabnetware Support
      Technical Support Forum for Cabnetware Users
    • OMEC/Macoser Inc
      Exclusive Importer of European Woodworking Machinery Since 1988
    • CabinetCRUNCHER
      3D Cabinet Design and Construction Software Powered by SketchUp and Excel, Precise Cut List Calculators with Highly Adjustable Construction Options for Cabinetmakers and Woodworkers of All Levels
    • J&P Machines
      Design and Production of Custom Equipment for the Manufacturing Industry
    • JKL Machinery
      US Exclusive Importer Casadei, Busellato, Vitap, Bonacin - Machinery Dealer representing New & Used Woodworking Machinery
    • WalzCraft
      Custom Doors and Wood Products

    Become a Sponsor today!