Sawing and Drying

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject:

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

drying wood in a hot box

6/27/17       
BigJim

Website: http://bigjimsbowcompany.com

I am trying to dry wood from around 10% or less to near 0% or as close as possible for stabilizing.
The wood sizes are typically 2" x 2" x 18" or slightly larger and the hot box's are capable of reaching temperatures of 180*-190* and stored outside.... Location is South Georgia and operating throughout the year.
Will I need to add fans in addition to the vent holes in the cabinets? Will I need to increase the temp to above 212* to bring the mc low enough to achieve below 3 or 4%??
I had been baking the wood in an actual house hold oven at 220* for as long as 6 and sometimes 7 days to achieve desired affect, but the oven only holds about 20 blocks whereas my new to me industrial kitchen warmer will hold 100 or more.

Any advice on where I might go to find the answers to these questions would also be of great help.
Thanks, BigJim

6/28/17       #2: drying wood in a hot box ...
GeneWengert-WoodDoc

The humidity determines the final MC. Do you need 4% MC final (which does seem dry as most homes seldom go under 6% MC)? So, this means about 26% RH at 150 F. See DRYING HARDWOOD LUMBER in the archives here at WoodWeb, pages 16 and 17 for a complete range of data. High heat over 180 F makes wood brittle, darker in color and possibly weaker.

6/28/17       #3: drying wood in a hot box ...
BigJim

I'm actually trying to dry below 4% if possible. Once the wood is as dry as I can get it, I will be stabilizing it.
Any moisture left in the wood not only displaces the stabilizing resin, but has the potential of locking up the pump (been there done that).
Much of the wood is not structurally sound to begin with such as burls and spalted, but the stabilizing changes that considerably.
Thanks, BigJim

6/28/17       #4: drying wood in a hot box ...
Tennessee Tim  Member

Website: http://www.tsmfarms.com

BigJim, here's a link to one of the many stabilizing products... https://www.turntex.com/ FROM what I've looked into there seems to be a issue with many not getting their pumps and vacuums set-up correctly or doing in too much haste. NO I haven't actually done any yet BUT I've been reading up with the pros and cons getting ready to purchase a system.
BEAUTIFUL bows!!! I remember learning to shoot my first bow in scout camp 40 yrs ago on a traditional style bow. I've shot and hunted when time allows , natural with no sights or releases.... it is on a compound now BUT I miss the traditional feel.

6/28/17       #5: drying wood in a hot box ...
Tennessee Tim  Member

Website: http://www.tsmfarms.com

I forgot to ask what system are you using and how its set-up?? How are you prepping the wood prior final drying??? ADing , KDing, straight off saw etc., etc.

Check out my website, I saw the odd stuff and there's parts I could stabilize for more productivity/ less waste.

6/28/17       #6: drying wood in a hot box ...
BigJim

Website: http://Bigjimsbowcompany.com

Nice work there Tim.
I've been successfully stabilizing wood for a little while. Yeah, I have had a failure or two also but that's part of it.
I'm running up to 8 tanks at a time but having trouble keeping up with the supply of dry wood.
I have lots of wood from all over the world waiting...hard soft , even mildly rotten, but don't have the time to load and un load a little oven ...not to mention the baby sitting because of the high heat (relative). Accidentally burnt up $500 worth of exotics when the spalted caught on fire in the oven.
Took everything but the oven with it.
Thank god this stuff is all outside my shop.

That is why I was hoping I could load this warming oven with a 100 or so pieces of wood. Turn up the heat to 180 or 190
..that is the max and let it dry for a couple weeks or even a month or so. I could even reverse the fan to draw air out.
If it worked, I would buy two more units so I would always have dry wood waiting for stabilizing.
Thanks, bigjim

7/23/17       #7: drying wood in a hot box ...
Gene Wengert-WoodDoc

Drying wood that hot can reduce the strength. It also makes the wood more brittle. Of the various stabilizing products I have been acquainted with, none require or perform better if the wood is dried to the level you indicate.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)