Sawing and Drying

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject:

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Equipment selection on dry kiln for wood

5/17/22       
Tim Heming

This question is for either Professor Wengardt or others that have expert advice regarding building a kiln enclosure to finalize moisture content to 8 percent MC and to sterilize the wood for insects. I started building this kiln using an old steel pallet rack because it is rated to handle weight and will be easy to move if needed. I have read information from the Drying Eastern Hardwood Lumber, the U.S. Forestry dry kiln build and also studied the Nyle's plans on dry kiln enclosure. I have a few questions concerning insulation, type of fans and CFM required, and what type of heat source and dehumidifier would be needed to bring down the moisture content.
First on insulation, the inside floor has 2 layers of 2" Dow XPS foamboard at R-20, 6 mil vapor barrier, 3/4 plywood. Walls are Johns Manville brand 1 1/2" Polyiso foil faced foam board which is rated at R-9.3 and the ceiling will consist of the 2 layers of the same foam board as walls but 2" and rated at R-26. Should I cover this foamboard with 6 mil visqueen before I apply the 4 mm Alucabond brand aluminum clad sheeting? Also I wanted to add more insulation to the walls on the back side to increase the R value by using either R-13 fiberglass batt which is cheap, or continue to use a thinner foam board to get the R value up past R-13? I know Professor Wengardt has mentioned about moisture getting past the surface and possibly getting into the insulation, so should I stay away from using fiberglass batt or open cell styrofoam even if I use a vapor barrier on the inside?

I plan on using this kiln to dry walnut and other more valuable wood for using in my cabinet/ woodworking business and selling the material to the public, so sterilization is the main reason for this kiln. I have in operation a solar kiln that was built in 2010 using the plans from Pro. Wengardt/Virginia Tech, and this has worked extremely well over the years in fact I am just finishing my kitchen cabinets that were built from shagbark hickory that I milled off my property.

Next on equipment, because this is such a small kiln, I wanted to use the Nyle L53 but because of "supply chain issues" they only offer the Nyle L200 which is more than I want to spend and to large for my needs, same goes for the EB LD800 that the plans that Neal Bennett designed for the U.S. Forestry. So I am looking at commercial grade dehumidifiers that are designed for crawl spaces and using monitoring systems like the Ink Bird brand that has been mentioned before on this site. The wood going into the kiln will be 8/4 walnut wood slabs 20" to 32" which is maximum width for my TimberKing 1600 to cut. Length will be 10' or under. I won't go into detail on stickers and the like because I have been reading the Drying Eastern Hardwood Lumber handbook. This walnut or other species will be air dried/solar kiln dried down to as low as I can get it for the the relative humidity in the Michigan area then finished drying to 8 percent and sterilized for bugs.

Fans, how many and how much CFM? For a 4' wide x 12' long x 7' tall chamber I want to have good circulation but not to much to overpower causing drying problems. Should I use 3 fans hanging centrally positioned off the ceiling with 12-16" diameter blades and should these fans be reversible in air movement? Also the need to cool the chamber down what size of intake and exhaust vent and should this be motorized on the exhaust side?

Heat source, I am not really planning on using this during the winter months in my pole barn because it is not heated. But during the summer months it can get warm inside the barn and this may possibly overheat the kiln. Should I be concerned with heating the inside? I have seen many plans using heat lamp bulbs, halogen work lights, or space heaters. During my high school days in wood shop I made a fiberglass re-curve bow that was placed in a plywood insulated box that was heated with an ordinary 150w incandescent light bulb and a muffin fan to circulate the air, this was back in the 70's. So this "Hot Box" should not need to much of a heat source to raise the temperature during the summer months inside the kiln. With that said, should I remove the dehumidifier once the desired MC in the wood has been achieved so that it won't overheat during the sterilization cycle.

Thanks in advance for input and advice.


View higher quality, full size image (4032 X 1960)


View higher quality, full size image (4032 X 1960)


View higher quality, full size image (4032 X 1960)

5/17/22       #2: Equipment selection on dry kiln for ...
RichC

I don't see any plans for sterilizing the wood. You'll have to bring the kiln up to around 150 degrees to get the centers of the slabs up to 133 degrees to kill all stages of bugs. That's after the lumber is dry.

5/17/22       #3: Sorry, reread and I had skimmed ove ...
RichC

Just make sure your heat source meets the temps I mentioned,

11/3/22       #4: Equipment selection on dry kiln for ...
Tim Heming

Update on my Dry Kiln: It has been a slow process constructing this but I am happy to say that completion is around the corner. Busy gathering logs and cutting them on my mill have taken me away from this project and placed it on the back burner.

I finally decided to purchase the Nyle L53 kiln unit and will be taking delivery on this in a few days. I have basically followed the design plans of the Nyle kiln chambers construction plans.

Thanks for all the input on this.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Baker Products
      Industrial Woodworking Machines, Wooden Pallet Manufacturing Machines, & Portable Sawmills
    • Rose Machinery
      Horizontal Band Re-rips, Standard & Custom Designed Machinery

    Become a Sponsor today!