secondary heat source for solar kiln

2/8/15       
Doug Simpson Member

I intend on building a solar kiln to hold 10,000 bf, at the same time I will be building a shop and using a wood boiler to heat the concrete floors. My question, has anyone used a heated floor as a secondary heat source in a solar kiln?

2/8/15       #2: secondary heat source for solar kil ...
Gene Wengert-WoodDoc

You would have to have a solar kiln that is essentially a closed room with a separate collector. The reason is that a solar kiln of the semi-greenhouse design has tremendous heat losses in the evening, night and early morning. So, a separate collector would have to be about 1000 sq ft for a 10 MBF kiln. a sep[arate collector will cost about $30 per square foot, so you would be looking at $30K just for the collector. At that cost, you would be better off with a DH kiln.

2/9/15       #3: secondary heat source for solar kil ...
don lewis

Website: http://nyle.com

Radiant floors are a bad idea in kilns. To work the temperature of the floor always has to be warmer than the air. And you can only get about 100 BTUH per square foot of radiant floor so that isn't much. Also you can damage the bottom courses if it isn't carefully controlled. Some tests have shown that solar kilns use more electricity than dh kilns because the slow drying means the fans run a long time.

2/9/15       #4: secondary heat source for solar kil ...
Doug Simpson Member

Thank you to both of you for your wisdom. I buy timber for a local mill and know logging and timber very well, but when it comes time to turn logs into lumber I am pretty dumb. I am nearing retirement and want a small business milling logs from my tree farm (700 ac.+/-).

2/9/15       #5: secondary heat source for solar kil ...
Gene Wengert-WoodDoc

Doug,
Your retirement idea is indeed a good one, BUT...

You will get more income and more profit if you do kiln dry the upper grades.

You will find that oftentimes and maybe always, you will spend more time marketing and selling than sawing and drying. In fact, you can saw all day, every day of the week, but you only make money when the lumber is sold.

In your business, there will be times when you need cash (sales are slow; a good deal for some logs comes up; maintenance, etc.). So, always keep as much cash as possible and buy equipment using credit or a loan from the bank. Small business groups in the state may be able to help identify good sources of money; local banks are often excellent too.

Get a business plan that identifies who you are, what you can and will do, what you will not do, markets, and so on. Again, state small business people (often through the county extension agent) can help.

For equipment, buy equipment that someone else has already done all the research and testing. In other words, buy top name brands. Buy "Made in USA" for good maintenance. (For sawmills, choose a big company and the size mill that they sell which will work for you. Then use that piece of equipment to compare to everyone else's equipment. Use a similar approach for a kiln.) Visit someone nearby that has the same equipment and see it running.

Although the upper grades often can be sold easily and with reasonable profit, the lower grades (sometimes 40% of a log is low grade lumber, or more) must also be sold. Profit is less with lower grades, so do not spend lots of time with them in manufacturing or marketing. A business plan forces you to consider all these aspects in advance.

Consider purchasing a kiln first and having all the logs sawn by a contract sawmiller for you. This costs a little bit for sawing, but does mean that you do not have a capital investment and sawmill maintenance...or the mess of a sawmill - - bark, slabs and sawdust. Plus, with a kiln your labor will be less so you can go fishing during the day and then check the kiln at night.

With a kiln, check out a DH kiln that is in a well insulated reefer van. Lots of postings about that here, plus I believe NYLE has some plans (and they credit what the plans cost against any purchase you make). Again, I like something that I know will work, rather than something that I have to do some testing or engineering because the company has this new product, etc.

If you do put in a permanent kiln building, always think ahead and make sure its location is perfect; that is, should you double your size, check that the first kiln is not in the wrong place when you expand.

Contact your power company's business office and they can help you with the best rate for a kiln (which is running 24/7, which means low peak demand). I have heard that because a DH uses a heart pump, that there were some special incentives for that in at least one state.

Finally, join a drying association. Many meet several times a year and have both plant visits and technical presentations. Most have beginners classes too. There are active kiln groups in the Great Lakes, Ohio Valley, PA, New England, Southeast (VA, NC, SC, GA). Of course, you could hire me to come in for a day or two, but that is expensive...the best is always more expensive (LOL).

Attend a 3-day hardwood lumber grading class and also a 3-day drying class. You will also find that within our industry, your competitors are often very willing to share with you.

Questions?

2/12/15       #6: secondary heat source for solar kil ...
Heinrich Spillmann Member

Gene, it is truly great seeing you at work, dispensing wisdom and great advise and all for free, a voice of sanity in this crazy world of online “wisdom”. Thank you much, be well

3/1/15       #7: secondary heat source for solar kil ...
old 243

I agree with Gene, Take 3 day grading and drying courses. I did, you will identify the grade of your boards before they come out of the log. You will start cutting for best grade. That is where the dollars can be made. Leave the knots and defects in your narrow , low grade boards. I am a low volume cutter, purchased a nyle 50 , after I got my mill, You can keep your kiln going ,even if you don't have your own wood to do. There is a steady stream of people that want a few logs cut, then dried, Sometimes you will make just as much this way as they dry all their , boards not just the lower quality. Also I think you should probably undersize your kiln, make it suit what you intend to have for volume, and have it going all the time. If you can't keep up at a later date. add another kiln, rather than having too large a one and have it sit idle some of the time. I think I make more out of kilning as there is none in our area , people will find out, you have one and , come knocking. Good Luck


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Baker Products
      Industrial Woodworking Machines, Wooden Pallet Manufacturing Machines, & Portable Sawmills
    • Rose Machinery
      Horizontal Band Re-rips, Standard & Custom Designed Machinery

    Become a Sponsor today!