Target MC Reduction/day for Yellow Poplar

10/30/20       
George Barth Member

What is the target daily MC reduction rate when Air drying, Shed drying, or otherwise DH drying Yellow Poplar from Green to 20% MC?

First, I have researched (searched online) and read several of the USDA publications and will specifically reference FPL-GTR-117. Noteworthy, the 117 pub is a bit inconsistent.

Pub 117 References:
P. 2 Table 1 list green yellow-poplar at 83 to 106 MC. Let's use 95% MC for simplicity.
P. 24 Table 7 shows an air drying day range of 1" poplar to 20% MC from 40 days to 150 days...depending on environmental conditions. At the 40 day time, the daily MC reduction rate is less than 2%
P 25, Table 8 has similar times, but adds the 50mm thickness. again 40 days is the lowest time for 1" thickness.

P26, Table 9 it shows cases in Roanoke, VA where the lowest days is 14 or 15. Doing the math: from 95% (green) to 20% or 75%MC loss in 14 days is greater than 5% MC loss per day.

I assume no degrade from the listed references in Pub 117 and only limited by environmental factors (temp / humidity).

So what is the Maximum (conservative) MC loss per day of low temperature (70 degrees F) drying green yellow poplar to 20% without any degrade?

Any data out there or industry standards for Yellow-Poplar for the following thicknesses?

4/4
5/4
8/4
12/4

Thanks in advance,
George

11/7/20       #3: Target MC Reduction/day for Yellow ...
GeneWengert-WoodDoc

I believe you mean FPL- GTR-118.

I do not see the green moisture for yellow poplar in my copy of this text. Incidentally, the headings for this table are reversed.

Appreciate that the average MC loss does not give you the maximum loss rate. In fact, drying to fast at the higher MCs can create damage, even when the weather eases back and drying slows later. The average looks good, but a few days of excessively fast drying can ruin the lumber.

I think by calculating an average rate, you are misusing the original data. Further, the original data was for a specific location.

The maximum daily loss for 4/4 yellow poplar is similar to soft maple.

11/7/20       #4: Target MC Reduction/day for Yellow ...
George Member

Thanks Gene,
I definitely referenced Air Drying of Lumber, FPL-GTR-117 (Seven), October, 1999.

Reference the page numbers and Tables I provided in my original text. Again, I realize the rates are based on the environment, but the Roanoke data (at 5% MC loss in the aggregate) is what interests me.

My 8/4 load now is loosing about 3 to 4 percent MC per day( 50MC to 40MC). Measured in the center from Lignomat PK probes. I pin the outside as well daily and keep a log. I put the pins in about 1/16" and it reads from 15 to 20 MC at various points. So my differential has been about 20 MC from outside to inside.

I am intrigued by the Roanoke 15 day run and wonder if I control the shed conditions (lower the humidity) to achieve those results, will I surface check the Poplar?

I understand that it is way more relisient to high MC derivatives verses Oak. Just wonder what my target should be.

In your class on drying Oak, you give a 3 % MC loss max on 4/4 and I believe half that for 8/4.

what should the target be for Poplar?

Thanks again!
George

11/7/20       #5: Target MC Reduction/day for Yellow ...
GeneWengert-WoodDoc

The Air Drying book you called 117 is a revision of an earlier publication. Many of the photos and tables, plus suggestions are from forty to fifty years ago, so do not represent today's needs and reality very well. The current techniques are not well covered. For example, air drying yards are much more open over the last twenty years or so, so we do get faster drying. In the old days, the yards often had four eight foot wide packs stacked edge to edge, so yards dried more slowly. So, their yard layouts with lots of lumber ina small area are not realistic. Also, yellow poplar when 117 was written was not the premium species that it is now. I

I would rely more on FPL-GTR-118 as two of the authors had practical experience and worked with the industry daily so they saw many practical ideas. They also have appreciated the financial aspects of suggestions.

If you look on page 99, you will find the daily safe drying rate for 4/4 and 8/4 yellow poplar.

Appreciate that weather, air flow, stacking including pile width, and yard layouts are entirely different. For yellow poplar, sheds with fans are great.

11/7/20       #6: Target MC Reduction/day for Yellow ...
George Member

Thanks Gene,
That sheds light on the history and conditions and certainly the evolution of best practices.

I have 118 and and just reviewed that section. Thanks for that tip. That is exactly what I was looking for.

I was hoping to capitalize on knowledge that was out there so I do not turn the Dehumidifiers down too low and damage the loads.

Thanks so much, you are very helpful.

all the best,

George


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Baker Products
      Industrial Woodworking Machines, Wooden Pallet Manufacturing Machines, & Portable Sawmills
    • Rose Machinery
      Horizontal Band Re-rips, Standard & Custom Designed Machinery

    Become a Sponsor today!