Kelly Member

Rebuilding my garage/shop that was lost in the Santa Cruz fire last August. Doug Fir timber frame, with timbers ranging from 6x6 knee braces to 8x12 beams. Most elements are 7x7, 6x8, 6x10. Total BF is ~2,200, of which ~2,000 just started baking the past few days in a solar kiln we built a few weeks back from the VT plans. Kiln's net inside dimensions are ~22' long, 4' deep (front to back) and height ranges from ~4' to 8' in a ~37 degree slope matching our latitude. South facing, on a newly poured slab, sealed well and 2x4 + plywood walls insulated with R13 glass batts. Roof is dual pane polycarbonate sheets. 1" foam panels put on at night to help retain heat. Internals include on Honeywell residential 70 pint dehumidifier, one 1500W electric space heater, and four cheap box fans for internal recirc (two on each end). Exhaust fans on east and west ends of kiln, with gravity-driven vent flaps (closed when fans off, blown open when fans on). All electrical elements controlled by WiFi-enabled 110v outlets. Inside temp and humidity reported by WiFi-connected weather station indoor unit. Hygrometer going in tomorrow, as a check on RH reported by weather station unit.

I've read lots of the technical literature, studied the tables, schedules, recipes, etc., and would appreciate expert input on how many days or hours at various temp and RH settings. Goal is MC in the 9% to 11% range. Timbers milled within the past two months from DF logs dropped in late January, killed by the fire 4 months before being dropped. So to some sense they "air dried" before being dropped. Most are new growth, in the 24" to 50" diameter range. Several are old growth, with 200+ rings. My cheap $40 pin moisture meter says ~28% MC the moment my mill slices them open, and a couple months air dry stickered on the deck yields MC's ranging from 16% to 19%.

What other data can a provide to guide one of you black belts to recommend a "recipe" for achieving our KD timber frame goals?

Having a blast with this.

6/11/21       #2: Guidance for drying Doug Fir timber ...
Tennessee Tim  Member

Website: http://www.tsmfarms.com

Kelly, Gene may correct me BUT....
1) I think that MC goal may be incorrect for framing materials or from what I've read and heard. I think it's more a 18% range and that could of changed over the last few years. It would be too dry for most areas and regain to average MC of the area which equals more movement.
2) I've also read that the larger "kilned" timbers were bringing some MC down BUT more for the sterilizing (killing bugs) and sap setting part of "kiln dried" with the high temp. From my readings large timbers as 6"x6" and larger would required such a huge kiln time to appropriately dry that deep it isn't financially credible as thickness creates slower moisture removing time and gets slower every 1/4" you gain in thickness.
YES there are a few log claims for full kiln BUT....BUT..BUT my understanding is they start with standing dead AND still not positive dry to the core.
Happy cutting and building. Sorry for your losses BUT glad your still around to put back your dream.
I'm finishing up a timberframe install into a 20'x30' stud framed barn I wanted to salvage. IT'S been a challenge as everything was fitted into and not craned up. I actually lifted the whole barn to laser level using the bottom and main top beam plates and many come-a-long angle bracing as every inch lift required multiple adjustments.
What brand mill do you own??? I have a Cooks.

6/11/21       #4: Guidance for drying Doug Fir timber ...
Kelly Member

My mill is a Lucas 7-23 swing arm mill. I will also be milling and drying redwood (1" and 2" thick boards for decking, siding, etc.) and Valley Oak (a white oak) for trim, cabinetry, flooring, furniture, etc.

My system is entirely solar powered (other than the gas mill), so fans, dehumidifier(s), heater(s) all cost me $0. Forever. And I'm not in a terrible rush, though faster generally better, up to the point of wood damage.

I just put cheap $40 MC meter in the 8x8 posts in my Doug Fir timber frame in the home that survived the fire. It's been standing since 1994, and reads ~8.8% MC. All but a few of the large Doug Fir timbers I am milling will live inside, in same/similar climate as existing house.

6/11/21       #6: Guidance for drying Doug Fir timber ...
Tennessee Tim  Member

Website: http://www.tsmfarms.com

Those swing mills are amazing. I have the Cooks superwide 52" mill with 20' cut length.
I had a Hud-son Farmboss 36 with 24' cut bed prior. LONG timbers require special equipment to handle those lengths.

I can understand the house frame being 8.8% now, but I'd be curious when it was stood up the true mc was.. We also have to understand we're measuring skin MC and not core. The house would most likely be that to the core as 26 years to gradually balance out is a LONG time to dry!!!
Good luck with the project and keep us/me posted on the progress.
Thanks,
Tim


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Baker Products
      Industrial Woodworking Machines, Wooden Pallet Manufacturing Machines, & Portable Sawmills
    • Rose Machinery
      Horizontal Band Re-rips, Standard & Custom Designed Machinery

    Become a Sponsor today!