Solid Wood Machining

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Stroke Sander: Good for finish sanding?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Stroke Sander: Good for finish sanding?

12/23/13       
Joshua Johnson Member

Website: http://www.jaaronwoodcountertops.com

I'm thinking of getting a stroke sander. Does anyone use one for full finish sanding or are they mostly used like an over sized belt sander?

12/23/13       #2: Stroke Sander: Good for finish sand ...
joiner Member

Joshua,
I am a big fan of stroke sanders for both heavy removal sanding and finish work. You will find however that many woodworkers are not so enthusiastic. Drum and widebelt machines have become the new rule for sanding, despite the higher expense.
The down side to stroke sanding is the high level of skill required to use it well. I had to teach myself how to apply the right pad pressure along with the right table movement to feather out the effect of the small pad without leaving obvious ruts, dips, and streaks. It took years of practice, but it is possible to quickly remove a consistent layer of surface leaving a uniform finished look. So, it's very labor intensive compared to poking it into a feed table.
Stroke sanding is also slower for production runs, as well as length restricted compared to the big machines.
Still, if you can get a bargain on a stroker, and like a challenge, it's a very satisfying and cost effective way to smooth a panel.

12/23/13       #3: Stroke Sander: Good for finish sand ...
Joshua Johnson Member

Thanks joiner. I think I'm going to give it a try.

12/23/13       #4: Stroke Sander: Good for finish sand ...
Adam West  Member

Website: http://www.surfprepsanding.com

The stroke sander is a very fine art form. Keeping the contact pad moving is an absolute must to avoid damaging the product.

Stroke sanders are capable of some of the best finish sanding possible. The wide contact surfaces really make for a nice long, shallow scratch pattern.

If you want to go that route you will need lots of patience and practice. Wide belts need a lot less practice and patience.

12/25/13       #5: Stroke Sander: Good for finish sand ...
Joshua Johnson Member

Thanks for the feedback guys. I really appreciate it.

12/25/13       #6: Stroke Sander: Good for finish sand ...
joiner Member

Since you're interested, there are some points worth mentioning. Many stroke sanders are equipped with a pad attached to a mechanical control arm. I have never been able to use these with success.
The only way I know to really control the pad is with a handheld unit. Frankly, I think the mechanical pad is a failure of design. Probably the manufacturers offered it as an upgrade e$tra option. Also it keeps the hands away from the danger, and the danger is real. A fast moving, free floating sanding belt edge will severe digits like a knife.
The pressure pad I prefer is a shop made hardwood block with arched handle, centered lengthwise. The width should be about an inch shy of belt width, and length of around eight inches. Pad surface is graphite impregnated canvas, stretched both ways, and thoroughly tacked around all edges.
This pad gives the mechanic total physical control of the applied pressure pattern. As the belt rapidly passes at the work point, it will cup in a way that forms a long moving canoe like trough. This can seem like an annoyance at first, but is a real asset to the operator. Table movement pushes material perpendicular to the belt/ pad contact area. If the pad is held to the belt so as the upturned edge of belt is on the leading contact of the wood, the belt will ride smoothly over the surface, even on a frame and panel door.
Sometimes when starting a fresh graphite pad, the belt back will overload with new graphite to a degree that the drive wheel will begin to slip, and too much pad pressure will stall out the belt. This is just a part of breaking in a new pad. Simply get out the lacquer thinner, load up a rag, and wipe down the back of the moving belt against a waste piece of wood. Watch those fingers!
As for technique. It's the old patting ones head while rubbing the tummy, and you have to rub the tummy in a very certain way. Once it's grasped, it really is like riding a bike. except for the amputation part.

12/27/13       #7: Stroke Sander: Good for finish sand ...
Bruce H

I have several pads for my stroke sander. a finish pad with some dense foam and graphite glued to it and a rough pad made out of 1/2" steel with graphite glued to it. depending on the product you can do things with a stroke sander that you can not with a widebelt. check out you tube and the making of coffered lids for caskets using an automated stroke sander to sand the curved lid. something not possible with a widebelt.

12/29/13       #8: Stroke Sander: Good for finish sand ...
B.H. Davis Member

Years ago I had a Boice-Crane metal working stroke sander in the shop. There really isn't much difference between a metal working and wood working sander. I think it was more a matter of work surface size and max. height limitations.

I sanded hundreds of cabinet doors with that sander and didn't stop using it until I got my wide belt. It was enjoyable to use and I miss having it around as it didn't make the trip to a new shop somewhere along the way.

A couple cautions:

1) As mentioned above stroke sanders can be dangerous. There is really no way I know of to guard the belt edge and so it is exposed as it flys by your hands. Be very careful and don't become complacent as you become more competent with the machine.

2) When sanding cabinet doors it is very east to drop the belt edge off the door stile and into the panel recess. When you pull or push the table back in the opposite direction the belt edge can carve a slot in the inside edge of the style. Repairable but a pain.

BH Davis

1/1/14       #9: Stroke Sander: Good for finish sand ...
Joe Calhoon

I acquired a lever pad Samco stroke sander when starting out over 35 years ago. I would disagree the lever action is poor design. It is just a different skill set from the hand pad and a lot safer.

Not everyone can run one and takes a very light touch to not destroy work. As BH says they are a pleasant machine to operate. We used to sand batches of interior, exterior and cabinet doors on the machine.

No doubt the wide belt is better for most work and the downside is the huge amount of real estate they take. We ended up selling ours because of this.

Early on we had PVC dust collection pipe (not recommended) When sanding a large batch of doors your hair would stand straight up when walking under the pipe extracting the sander.

Joe

2/24/14       #10: Stroke Sander: Good for finish sand ...
Rick L  Member

Stroke sanders are the least appreciated and the most misunderstood machines. Very fine finishes can be achieved with them. One time we sanded a veneered panel 4 times because the finishers couldn't get the stain right and still salvaged the panel. The lever type are called fulcrum pad stroke sanders and are perfectly designed as such, They definitely are more efficient then hand block sanding if spending 8 hours at a time on the machine.

I consider myself and expert on the machine having worked with them for over 40 years in metal and woodshops. One shop we had 3 stroke sanders and 1 widebelt. One stroke sander had flexible "J" weight belts and we used a graphite glove for sanding contours. http://www.pecfrictionfighters.com/product.aspx?prodID=65 This is the go to source for graphite...

The other sander had a pneumatic platen that was lever operated and the third stroke sander was a double belt through feed model.

Few people know how to properly make a handblock pad. You can somewhat teach yourself to use a stroke sander but you will never master the subtle details. I learned from a 40 year veteran of the stroke sander. The best handblock is a hollowed out and the hollow is filled with lead or steel. Underneath the graphite canvas is a piece of 1/4" firm felt carefully manicured with a 1/16" taper on the edges. The same holds true for a handblock or fulcrum pad sander.

It takes a lot of practice to master it and it's especially true of the fulcrum pad sander. I know pf one high end shop that had a stroke sander and could never figure it out and finally got rid of it. Because they are so minunderstood they are often priced at scrap metal prices. I brought a stoke sander in a custom metal shop that thought there was no machine that could duplicate their hand sanded finish. Boy were they wrong. There's a place nearby that does bronze plaques and uses a stroke sander to smooth the face of the plaques.

6/7/14       #11: Stroke Sander: Good for finish sand ...
Gary B.

I second everything Rick says above, he's spot on. I've used four of them in my career, including a double belt machine. Used on high end conference tables. Once you get the skill, you can sand any veneered panel with confidence.

I wish we still had one. One thing I will say is think "OLD IRON"; the bigger or older the machine, the better. I'm not impressed with any of them from the '80s on

2/13/24       #13: Stroke Sander: Good for finish sand ...
faith Amert Member

Website: https://glumber.com/

Grothouse has made a name for itself in the interior design and fine furnishings industry through its unmatched craftsmanship, inventive solutions, and trend-setting designs. Recently, Grothouse’s influence has been prominently showcased in various industry publications.

4/6/25       #14: Stroke Sander: Good for finish sand ...
Kyle Member

Hey Guys, we have a Samco Stroke Sander Model LLT. 5x10 foot table and 6" wide belts.
No clue the number of belts.. But MANY grits and even lots of felt ones of different densities, presumably for polishing. Most of the belts are new.

I have never used it, it was disconnected before we moved in. But I do know it was working before it was disconnected.

Anybody interested? Mostly just want it out of my way. Located in Abingdon VA. Reach out by email.

12/10/25       #15: Stroke Sander: Good for finish sand ...
henrycollins Member

Stroke sander is great for leveling and processing large surfaces, but it's not smooth enough for a complete sanding finish. I still have to use additional orbital sanders or hand sanding to achieve the desired finish before painting.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)