Solid Wood Machining

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Which 26"-32" Thickness Planer for various kind of woods

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Which 26"-32" Thickness Planer for various kind of woods

7/15/16       
cct Member

Hi all, I am asking your expert experience:

Please recommend a low cost, easy to use heavy duty planer for me. ;)

I need
a) 3-4mm cut in a single pass
b) as high speed as possible
c) Traditional planer blade
d) Heavy duty, can plane at least 10 ton of hardwood in a single day without stop.
e) Super easy to install blade.
f) Hardwood with different moisture content
ty

7/18/16       #2: Which 26"-32" Thickness P ...
tcc

Thickness planer? Isn't the wood already thick? Do you want to make it thinner? You need a thinness planer.

If one is a ton, would not ten be "tons"? I ask because I want to understand why you don't just buy a planer and start running it.

As for a magical machine that will never break down - buy Chinese.

7/19/16       #3: Which 26"-32" Thickness P ...
cct Member

Dear experts,

I mean i need to plane 10 X 1000kgs of wood everyday.

Which 26" heavy planer is recommended. One side is enough. 15HP minimum for traditional blade.

Thanks very much.

7/19/16       #4: Which 26"-32" Thickness P ...
cct Member

Dear tcc,

I already bought a china made planer, it break down (component burnt but easy to replace) almost everyday.. ;|. I need to give the machine a few breaks throughout the day...

But I still prefer china made or taiwan made planer because they are a few times cheaper. Please recommend a good machines for me.

7/19/16       #5: Which 26"-32" Thickness P ...
Bill Braskey Member

If you have a way to move 10 ton of lumber get a USA made planer that weighs at least 3 ton...

7/20/16       #6: Which 26"-32" Thickness P ...
ctc

Get a kraut machine - they are able to process wood using the metric system.

If that doesn't work out, try building your own.

7/20/16       #7: Which 26"-32" Thickness P ...
bb4

All this and, "low cost" to boot?

7/21/16       #8: Which 26"-32" Thickness P ...
cct Member

Dear experts,

Our stock is different from the stock in Europe. Our stock soak in water for long term and form very hard "skin". 1 ton or 1000 kg, only contains about 80 or less pieces of 8" X 7' stock or even less for stock that is 15". 10 Tons or 10, 000kg of stock only has 80 X 10 = 800 pieces of 8" X 7'. If a heavy duty can't perform the job, then the machine should not called as "heavy" duty.

7/21/16       #9: Which 26"-32" Thickness P ...
cct Member

7 Feet is about 2m. Heavy duty planer can plan around 9m/minutes. That means 1 minute can plan about 4 pieces.

1 Ton or 1000 kg, or 80 pieces of stock, only needs 80/4 = 20 minutes.

10 Ton or 10,000kg, 20 X 10 = 200 minutes or 200/60 = about 3 hours.

Reasonable? Most european stock looks extremely lightweight in youtube.

7/21/16       #10: Which 26"-32" Thickness P ...
Kilgore Trout Member

Your math is OK, but that is only one pass thru the machine. If you are going from rough sawn to finish, each side may get 2-3 passes thru the planer.

If 2 passes per side, multiply your numbers by 4.

What are you doing with the lumber after planing?

Heavy duty is a subjective term, not a defined term. China is not known for accuracy in their machinery descriptions. One man's heavy duty is another man's lightweight. Good used equipment is available easily in the US, but I do not know where you are.

7/22/16       #11: Which 26"-32" Thickness P ...
David R Sochar Member

None of my business, but why is he planing lumber at the source? Generally, logs are hauled to a sawmill, and sawn, then taken to a collection point where they are put on stickers to partially air dry (PAD), then moved to transport for export, or dried in a kiln, then exported. Planing does not happen until the wholesaler or retailer does it, if then.

7/26/16       #13: Which 26"-32" Thickness P ...
cct Member

cutterhead diameter 98mm
cuttinf circle 101mm
what ia the maximum planing depth?

ty

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)