Solid Wood Machining

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Dovetail Machines....

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Dovetail Machines....

5/16/17       
Leo G Member

Thinking about moving up from the smaller manual dovetail jig up to a dovetail machine. Shop Fox, Powermatic, Cantek, Hoffman all make these machines. Looking for one of the manual ones as they get pricey quick.

Seem to come in two flavors, 11 1/4" and 16". Big price jump from the smaller to the bigger one.

Anyone have experience with any of these? What to look for, what to stay away from. Sources to buy (I'm in the North East).

5/17/17       #2: Dovetail Machines.... ...
Robwood

Check out the Dodds, I've been happy for years with it

5/20/17       #3: Dovetail Machines.... ...
Andrew J. Coholic  Member

Website: http://www.joecoholiccustomfurniture.com

We used a few of the old cast aluminum Porter Cable DT jigs for years... three years ago I bought a Cantek JDT65, and it has been very nice for our shop (custom wood furniture and cabinetry, we do several hundred drawers and trays yearly but not production).

Anyhow, other than the addition of a PCD bit (from Royce/Ayr) so we can do Baltic birch as well as hardwood, it has proven itself to be a step up from the router & jig for sure. The pneumatic hold downs are excellent, the machine is easy to use (takes a few runs of drawers to get used to moving the cutter around the template, and getting quick at placing the parts in and swapping sides etc but after a few times its easy.

Since were hooked up to dust collection, no no more mess either.

I am glad we went with the 16" unit as we do deep boxes often enough.

Heres a link to the site - they actually linked my Youtube video I made as soon as I took delivery of the machine back in 2004.

Manual Dovetail Machine

5/20/17       #4: Dovetail Machines.... ...
Leo G

I had looked at that machine along with a few others. Ended up going with the Grizzly G0611X which is the 16 1/2" machine.

I've seen reviews that the bit that they sell for their machine breaks easy and one of the owners had found that the Omec 750 Single Flute Dovetail Bit solves this problem.

I do 95% Baltic Birch boxes. Am I going to have issues with the cutter?

One of the main reasons I went up to the machine is my Reliant Dovetail jig uses a 1/2" 14º bit which I break often enough that it is annoying (to say the least). I get pretty good result otherwise using a standard 2 flute bit. Sometimes a bit of the pin breaks off because the lamination fails, but since it's hidden inside the socket it doesn't really matter that much.

5/20/17       #5: Dovetail Machines.... ...
Andrew J. Coholic  Member

Website: http://www.joecoholiccustomfurniture.com

Baltic birch is a lot harder on bits than solid wood - the diamond cutter will just last longer, thats all.

The single flute cutter is easy to set up, and seems to cut just fine. I always do a light climbing cut to sever the face fibers, then do my full cuts from left to right.

The Cantek and Omec single flute are the same physical size, yes. I used a few of the Canteks before switching last year to the PCD. No breakage issues.

5/20/17       #6: Dovetail Machines.... ...
Leo G

Any chance you could give me a cost on the PCD bit?

The Omec was $69 but the shipping was $22, so it really cost me about $90 for the bit which was a bit hard to chew on. The Grizzly bit was around $35.

Not even sure if the machine will come with a dovetail bit, it didn't give a "what's in the box" description.

5/20/17       #7: Dovetail Machines.... ...
Andrew J. Coholic  Member

Website: http://www.joecoholiccustomfurniture.com

If you thought the Omec was steep... you will have to cough up about $250 for a PCD bit. But, look at it this way - they claim dozens of times more life than carbide. Its no sharper, but should stay as sharp as a fresh carbide bit for a long time.

I'd have to look up my invoice, but I am sure it was somewhere in the $250 C range..

At the IWF show last August, I talked to several companies who manufacture tooling about alternatives for the stock single flute DT bit. Not much else made besides the brazed carbide. I decided to try the diamond, and so far its working fine. Leaves a bit of fuzz on the tails cut, in the rounded portion but that comes off quickly when we presand the sides before assembly. Only on solid wood though, Baltic cuts fine.

5/20/17       #8: Dovetail Machines.... ...
Leo G

How about prefinishing before cutting the dovetails? Would it work, or no matter what you'd be putting another coat on the exterior.

I know it'll work for the interior of the drawer, not sure about the exterior.

5/20/17       #9: Dovetail Machines.... ...
Andrew J. Coholic  Member

Website: http://www.joecoholiccustomfurniture.com

I never cared for prefinishing - you either leave the end grain of the front/back unfinished, or touch it up. Plus there is always some small filling to be done. EVen with the high end CNC dovetailers, if you want perfect looking joints it is necessary to finish after assembly, sanding, etc.

We assemble, sand and finish our drawers with two coats of vinyl sealer, two top coats after buffing of post cat lacquer.

5/20/17       #10: Dovetail Machines.... ...
Leo G

Thanks, sort of what I figured. Had to ask.

5/26/17       #11: Dovetail Machines.... ...
Adam

Leo,

How many boxes has your old Reliant put out? I remember those blue ones from the woodworker's whorehouse days. We had one for a year or so and the template broke. We moved on to the better Porter Cable ones. That had to be almost 20 years ago.

5/26/17       #12: Dovetail Machines.... ...
Leo G

Probably thousands. Still going strong. The router bits are the weak point in that system.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)