Subject: Re: Re: Re: Re: Choosing wood species for laundry rack design

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Choosing wood species for laundry rack design

7/25/08       
Greg Baka Member

As an addition to my current business I will be producing a new design of a wooden laundry drying rack. Estimated at 1000 per year to begin with. I will outsource the component fabrication and just assemble and package here - and market, the toughest job.

I need suggestions on the species of wood to use.

We HOPE to use a raw unfinished hard wood. Here are the parameters the wood must meet (in it's raw but sanded condition):

1) must not bleed color onto damp fabric hung on the rack.

2) must easily sand smooth enough to not snag on silky undies or pantyhose, and not become rough from being dampened.

3) must not warp excessively as it absorbs and releases moisture from the damp fabrics

4) needs to be a fairly stiff and strong wood

5) needs to be a wood that is commercially converted into long dowels. This is tougher than it sounds as the dowel manufacturers all seem to cover the same half dozen or so species. But some will do other woods if the stock is readily available.

I have done some research and have a few species possibilities. But I would like to hear your unbiased thoughts first. I'll share what I found and the end of the thread.

Thank You!

7/30/08       #2: Choosing wood species for laundry r ...
Leo

I would say hard maple. But I think you will find that without sealing the wood and putting it into a high humidity environment you are going to be asking for problems. Plus you are putting damp articles of clothing on it. Any wood will have its grain raised by doing this which may lead to snagging of fine garments. Good luck with your quest.

8/2/08       #3: Choosing wood species for laundry r ...
Frank Pender

The more tradational has always been Douglas Fir, here on the Left Coast.

8/5/08       #4: Choosing wood species for laundry r ...
JJ

Bamboo

8/5/08       #5: Choosing wood species for laundry r ...
Adam

light brown PVC with a nice faux graining pattern. Kinda like a fibreglass door.

Other plastics may be more suitable for this product. I could list alot of woods that wouldn't be suitable.

8/5/08       #6: Choosing wood species for laundry r ...
Greg Baka

Definitely want wood. Too much plastic junk out there already. Bamboo is an interesting idea, but I don't think you could do the sort of drilling/notching/fabricating that we need.

We have pretty much narrowed the choices down to hard maple and white birch.

Now I need to do some testing to see how they behave when hung with wet fabrics.

Keep those ideas coming! I appreciate the info.

8/6/08       #7: Choosing wood species for laundry r ...
Adam

Leo,

Those maple drying racks could be worth a ton of money. After a couple of years they might become spalted. Dry them out, seal up with your favorite clear coat, and sell them as fine furniture...

8/6/08       #8: Choosing wood species for laundry r ...
Greg Baka

Hi Adam,

Excuse my minimal wood knowledge, but I can't tell if your kidding about the hard maple rack idea...

What is spalted? Is there something I should know about hard maple and what happens when repeatedly dampened and dried?

Thanks!

8/8/08       #9: Choosing wood species for laundry r ...
Gene Wengert-WoodDoc

I do beliee that hard maple will become rough with the repeated wetting. You should consider basswood or aspen. Both are white and will leave no residue; both will not develop extreme roughness with wetting, both are weak, so the diameter will have to be increased a bit, but doubling the diameter means 4x strength or more; both will have little warp if properly chosen wood

8/14/08       #10: Choosing wood species for laundry r ...
Ralph Member

Website: http://www.consultingwoodworker.com

Greg,

Bamboo most certainly can be drilled, milled, finished etc. to make what you describe.

Last year I did an article for Woodcraft Magazine on making bamboo sushi trays. Had great fun working with it. I was able to mill dovetail keys in the bamboo lumber with no difficulty

It can be had in "solid" form (glued up strips) in plywood and even in shapes.

Please check out my website, I would be happy to help you design and specify this product line as well as find and qualify possible shops to produce your parts.

Free free to contact me and we can discuss it further.

Ralph Bagnall
www.consultingwoodworker.com

8/14/08       #11: Choosing wood species for laundry r ...
Gene Wengert-WoodDoc

Bamboo can be a good choice for products that are not affected excessively by wetting and drying. Many bamboo species move more than oak. A cloth drying rack seems subject to wetting, so I am concerned that this is not a good use for bamboo.

8/14/08       #12: Choosing wood species for laundry r ...
Ralph Member

Website: http://www.consultingwoodworker.com

Not to argue with the wood doctor, but bamboo in it's lumber form is made up of a number of strips laminated together.

Bamboo is used extensively for cutting boards, and in baths for benches.

I had the opportunity to unscientifically test the waterproof qualities of bamboo lumber that was being considered for outdoor stair treads. Unfinished, I immersed it for several days. There were no delaminating issues. Three years hence the stairs in New England are holding up beautifully.

You may want to contact Chris at Northwest Bamboo. They sell bamboo lumber and he's been very helpful in answering my questions.

Ralph Bagnall
www.consultingwoodworker.com

http://northwestbamboo.com/index.html

8/14/08       #13: Choosing wood species for laundry r ...
Gene Wengert-WoodDoc

Thanks Ralph,
I have indeed done a lot of research into bamboo and had read studies done on the properties. Some species of bamboo (there are 1000s) behave pretty good, while others are terrible when compared to wood. Indeed, bamboo flooring and panels (not called plywood as bamboo is a grass and not wood, but one supplier calls them plyboo) are good some of the time too, but I have seen some terrible products.

You are indeed correct that bamboo is ripped into narrow strips and then glued together to make a flat product. Obviously, the type of adhesive is important if you want water resistance. In short, we do need to be careful that we say that all bamboo is equal...it is like saying all plywood is equal.

8/16/08       #14: Choosing wood species for laundry r ...
Ralph Member

Website: http://www.consultingwoodworker.com

Gene,

I can live with that. It is no different than plywood. Not all sheets are created equal. You have to be able to trust your supplier.

Ralph Bagnall

8/16/08       #15: Choosing wood species for laundry r ...
Gene Wengert-WoodDoc

Ralph...exactly.

I checked my records and I see that beech was used in the past as its grain did not raise. Perhaps that is also why it was used for wood clothes pins (if you are old enough to recall what they are).

2/10/09       #16: Choosing wood species for laundry r ...
Joe Redburn  Member

Greg Baka,
Heart of Cypress. I have seen fallen trees dug out of the mud in Mississippi that have been buried for 50 years or more and are still intact.
regards
Joe

4/4/09       #17: Re: Re: Re: Choosing wood species ...
Greg Baka Member

Website: http://www.bestdryingrack.com

It's been awhile since I started this thread. I wanted to thank everybody for your knowledge and let you know the final results.

We did finally go into production on the clothes drying racks. They are currently being sold through BestDryingRack.com (see the related link and picture)

We did end up using Hard White Maple. It looked nicer than birch, was stronger, and could be produced with a very fine smooth surface. We also use a soy-based wood sealer to prevent any raised grain issues.

I did find all US suppliers for the wood and steel, which was an adventure all on it's own. But definitely worth it. We have to help the small US manufacturers survive this downturn.

Maple was tough to find vendors for. The hanger dowels are 7/16" diameter and are actually made side-by-side 4 at a time on a molder. Evidently small diameter doweling machines are rare in the USA.

The laundry drying rack has been well liked by my customers. I really appreciate the knowledge and ideas you all shared on list and off. Thanks!


View larger image

Laundry Racks

4/4/09       #18: Choosing wood species for laundry r ...
Ralph  Member

Website: http://www.consultingwoodworker.com

Greg,

Thanks for the update, I have wondered how this all worked out.

Cool looking units.

Ralph Bagnall

4/4/09       #19: Choosing wood species for laundry r ...
Leo G

Website: http://lrgwood.com

Yer Welcome

Thanks for the update. Nice of you to remember to do that for us.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)