Subject: Re: Veneering a bullnose

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Veneering a bullnose

11/17/15       
Ted Member

I use my vac bags for laminating curved panels and have little to no experience with applying veneer. But I need to make a new shelf for some existing teak furniture as a favor to a customer. I want the 3/4" MDF shelf to have a bullnosed edge in front and my plan is to apply contact cement to the top of the shelf and the bullnosed edge. Then apply the veneer to the top with about 2 or 3" of veneer hanging over the front edge, put the shelf in the bag on some spacers that will hold it about an inch above the platen and press it. Once it is pressed I will turn the shelf over, apply some more cement to the bottom and the veneer flap and re-press. Does this sound like a reasonable approach? And by the way, the shelf will be low enough that the bare MDF on the underside won't be noticed.

11/18/15       #2: Veneering a bullnose ...
Max Neu

For something like that,I would use Heat lock glue.

11/18/15       #3: Veneering a bullnose ...
John Van Brussel

Website: http://www.veneersystems.com

Rule of thumb when veneering " what you do to one side of your panel you need to repeat on the other side." If you don't the shelf will warp or cup. Keep in mind if you use a PVA glue let it dry and reactivate it with heat you will weaken the bond by 50% or more.

11/18/15       #4: Veneering a bullnose ...
Ted Booth Member

Max,
I'm not familiar with heat lock glue. I'll have to read up on it but keep in mind what John had to say about re-heating it.

11/18/15       #5: Veneering a bullnose ...
Ted Booth Member

John,
I know what you say is true when regarding sheets of plywood I have custom ordered but I didn't think about that rule in this instance on a smaller shelf. Might have been to my peril. I have some maple veneer lying around from a previous instance that could do the trick on the unseen side. What about my idea for the bullnose, do you have experience with something like that?

11/18/15       #6: Veneering a bullnose ...
Geoff

Do NOT use contact adhesive. In my opinion, the best adhesive for this is Unibond 800. Like John said you must veneer both side of the panel.

11/19/15       #7: Veneering a bullnose ...
Ted Booth Member

Well I can see that the next thing I need to do is investigate all of my glue options. What I use for my curved panels is regular Tite Bond II which I apply using a Klebo spreader I bought from VacuPress about ten years ago. The Klebo for my purposes can't be beat. But veneer is a different animal. I went to Tite Bond mainly for the ease of clean up but I find that it works well too for all types of plywood and MDF glue ups.

Thank all of you for your comments. My original question still hasn't been answered but plenty of other issues have arisen that could cause problems which I would like to avoid. If you have more possible bad outcomes and ways to avoid them I would like to hear them before I get started.

11/19/15       #8: Veneering a bullnose ...
John Van Brussel

Website: http://www.veneersystems.com

Most bull noses I see are done separately and then glued and mechanically fastened to the shelf.You can do this in a vacuum press but you need to raise the piece so the bag gets the veneer pressed on to the bottom edges of the bull nose.

11/19/15       #9: Veneering a bullnose ...
Jared

I've done what you're trying to do, but it was awhile ago. If I recall, I used some kind of powdered plastic resin glue or epoxy. After putting the parts in the bag, I drew out a portion of the air, then used a hard roller to help the veneer make the corner. Draw out more air, more rolling, lather rinse repeat. Veneer softener is your friend.

11/19/15       #10: Veneering a bullnose ...
Ted Member

John,
I would like to have the veneer on the bullnose match that of the shelf so I'm going to try doing it all at once. But I still have the bullnose from the existing, too shallow shelf. If the job doesn't go right and the veneer on the bullnose bubbles or is otherwise ruined I'll rip the one off the old shelf and attach it on the new shelf. Also, as I mentioned in the initial post I plan on placing the shelf in the bag on spacers so that the bag will crawl under the shelf in the gap. This may be the only time I ever do want that crawl-under to happen.

11/19/15       #11: Veneering a bullnose ...
Ted Member

Jared,
I haven't used veneer softener previously. What I have is 10 mil veneer on paper. I would imagine that the softener is applied to the veneer side and not to the paper? Otherwise I can see the upside to stopping and rolling as the bag evacuates. Thanks for that tip.

11/19/15       #12: Veneering a bullnose ...
Jared

Ted, I've not used much paperback veneer so I can't attest to how it will behave with softener. My gut says the paper might inhibit the elasticity that would otherwise result, but maybe not to the point that it would be a hindrance to you. Raw veneer can be coaxed around compound curves with enough determination. I think my application was veneering the radiused edge of a round table. You've got a curve in only one direction, so it should be doable.

11/19/15       #13: Veneering a bullnose ...
Ted Member

Jared,
I would like to have seen what you did while it was happening. I do some compound curve stuff also but with plywood. It isn't easy.

11/25/15       #14: Veneering a bullnose ...
Tom Gardiner

By my reading of this, the bullnose wrap is not a compound curve. It is likely that the grain is running with the bullnose edge so the wrap with paper backed veneer should be relatively simple. Paper back is normally tenderized making it very pliable an not prone to stretching. Useless for compound curves but excellent for what you intend.
Try a dry run with veneer sized to wrap over the bullnose and cover the top of the shelf. Use a sheet of 6mil vapor barrier between the veneer and bag to reduce friction. Have the shelf raised up 1" or more. Tape the veneer in place and draw down the vacuum while massaging the bag into a tight fit around the curve.
It would help to have the shelf over length because the veneer will fracture as it gets pressed over the edges.
If this works the do the same with glue.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)