Veneer

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: RE: Old Wood Veneer

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

RE: Old Wood Veneer

7/18/19       
Tommy

What was the thickness of wood veneer in the 18th and 19th centuries, before the special thin slicing machines that we have today?

They are still in use as furniture, can I build with that thickness today and would it be a better product?

7/18/19       #2: RE: Old Wood Veneer ...
rich c.

In that time period they didn't have central heating and buildings were drafty. Some of the thick sawn veneers will not handle the shrinkage today. I've seen a lot of antiques with cracked burl and crotch veneer. Also completely missing pieces. There was nothing mystical about veneer in that time period.

7/19/19       #3: RE: Old Wood Veneer ...
David R Sochar Member

Before 1875, almost all veneers were shop sawn, using a veneer type saw - a frame saw. Veneer has been used, shop made, for thousands of years.

As the Industrial Revolution kicked in, veneer could be sliced economically and produced in large quantities. No rule, but 1/20th of an inch thickness was mentioned.

By 1900, many shops were producing casework of secondary woods, and then veneering them to doll them up. Using it like wallpaper does not work well. Pressing a veneer to a substrate in a wet glue line is the preferred way to glue veneers.

Unfortunately, the hide glue - the only commonly available glue at the time - was barely adequate for this kind of work. Especially if surfaces were not flat. When it let go, the owners invented 'curb furniture' - cheap goods that when failed, end up on the curb for pick-up by trash or whomever.

The link will take you to Capital Machine, one of the better machine makers. they have been making slicers in Indianapolis, IN since the early 1900's.

Capital Machine - Veneer Slicers

7/19/19       #4: RE: Old Wood Veneer ...
Tom Gardiner

Special thickness veneer is still available. 1/42" was the standard a few years ago. I'm not sure what export specs are today. Thinner veneer is possible not only because of the ability to slice that thin but also because manufacturers have the machinery to apply it and sand without sand through.
I have pressed 1/32" veneer and it is a treat. It is less apt to overlap in layup, you can edge glue it for stable joints and sanding is less stressful for me.
1/16" on the other hand is too stiff and prone to splinters. I have seen 1/24" advertised and would be the max thickness I would want to work with.

7/19/19       #5: RE: Old Wood Veneer ...
cbww

Machines to cut veneer were developed prior to 1850, both sliced and sawn. The American Empire period, around 1820, is when you start to see more veneered surfaces and maybe lower quality building practices based on cheap labor. The veneer was/is thicker on those pieces but not 1/16". What the actual thickness was will vary. Would thicker veneer make it a better product? maybe. I do like to use thicker veneer but the full 1/16" can be to thick at times for some applications.

Some of the veneers sliced today are just to thin. Hammer veneering, if you even do that type of work, is that much harder with thin veneers.

Hide glue is not a bad glue at all. Its just not the right glue for certain situations.

7/19/19       #6: RE: Old Wood Veneer ...
Tommy

I appreciate the above answers, but can a ¼ inch American hardwood of nice design be used as a veneer, or would it have to be less than a ¼, if so how much less?

The reason I am asking is because I have good looking hardwood pieces that are a ¼ inch thick, but they could be planed thinner if recommended.

Thank you.

7/20/19       #7: RE: Old Wood Veneer ...
Tom Gardiner

You are kicking at a hornet's nest. I do not consider 1/4" wood veneer. The reason veneer works is that the expansion forces of the veneer are kept under control by virtue of the small cross sectional area compared to the substrate. Once the veneer thickness is greater than 1/8" then the veneer starts to exert forces that make cross grain gluing or wide surfaces problematic.
There are furniture makers that saw thick 'veneers' and use them in pieces but they tend to be small scale and often skins on a floating panel.
I can't understand why someone would want to resaw his or her own veneers after looking at the selection available from numerous suppliers.

9/24/19       #8: RE: Old Wood Veneer ...
David R Sochar Member

There are rules, then there are rules. So, if 1/4" is to be thought of as solid wood, then what about these wooden building panels?

3 or 5 or 7 ply, with 2x materials, These panels should soon exhibit self-dectruction by all the logic we have amassed here at Woodweb. Multi-storey buildings are being built in some parts of the world with these. Yet they do not self-destruct - Why?

Plywood. The cross grain movement of the wood can be dramatic. Splitting off stone in a quarry, for example. It is hard to deny. Yet some folks do deny those cross grain properties and go right ahead making these panels.

Now I see them everywhere as 3 ply 8" x 10" panels used by utility companies to provide a clean, clear deck so their heavy equipment can work around without churning up mud. The panels arrive in a stack about 6' tall, and the three-ply panels are lifted of by a fork lift and distributed around.

Cross Laminated Timber

9/24/19       #9: RE: Old Wood Veneer ...
David R Sochar Member

A better way to get the image....


View higher quality, full size image (1024 X 593)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)