Wood NetWork

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Testing moisture resistance in particleboard

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Testing moisture resistance in particleboard

2/26/13       
Sean Member

We have a customer that wants us to use moisture resistant PB for cabinets. Our supplier has the moisture resistant PB but we want it tested by SGS to make sure it is.

I am not familar with how it is tested. How is the level of moisture resistance measure? For example density is measured as KG per cm3, so what is the unit of measure for water resistance and what type of tests establish this?

Also based on the unit of measure, what are the different levels of moisture resistance. For example at what level could a panel be described as HMR? (high moisture resistant)

Also any other information would be helpful such as any ANSI or EN standards that deal with moisture resistance in panels.

2/27/13       #2: Testing moisture resistance in part ...
David R Sochar Member

Website: http://www.acornwoodworks.com

Moisture resistance is a relative - subjective - term that is not measured or quantified by any accepted method. It is mostly a marketing term to add value to a different formulation of the product that fails in water at a slower rate than the 'normal' product.

As one engineer told me "Toilet paper can be called water resistant".

If the cabinets are to be subjected to an unusually high moisture environment, then alternate materials should be used. Consider those for exterior cabinets, marine use, etc.

2/27/13       #3: Testing moisture resistance in part ...
Sean Member

That's interesting. So if our customer asks for some type of guarantee or warranty that the PB is "moisture resistant" I'm not sure how we're going to go about that if it can't even be measured by SGS. I presume moisture resistant PB would do better in a "boiling water" test than normal PB?

2/27/13       #4: Testing moisture resistance in part ...
David R Sochar Member

Website: http://www.acornwoodworks.com

Two things: You can ask your vendor to supply whatever documentation he has on 'moisture resistant' materials, but you won't get much.

And - your customer is fixating on this for some reason. You can try to find out what their bad experience in the past was and address that, or politely move on and let them find another maker.

Most likely they had a slow leak in a sink cabinet and the PB sagged and got nasty. Sell them a phenolic floor and sides and back for a sink cabinet, and fix their plumbing. What is wrong with plywood?

You do not want to guarantee any further than your supplier will guarantee. All he will do is document that the product is indeed labeled as 'moisture resistant' and nothing more.

I don't know who SGS is, and if they deal in finite metrics, fine. But who will pay them to determine objectively what is essentially a subjective phrase? Would they determine if blue or red is a better color? Sounds like a great gig if you can get it.

2/27/13       #5: Testing moisture resistance in part ...
Sean Member

David,

Yeah SGS are an inspection/testing company.

Its defiantly difficult to guarantee the moisture resistant PB for a period of time if there is no test for it. If we guaranteed it as being moisture resistant for 10 years, what would that even mean and how would one prove it stopped being "moisture resistant".

Sounds like a difficult one, but our customer is insisting on tests/guarantee/warranty. Its around $300 to carry out the test with SGS, but as you said not sure what that would entail.

2/27/13       #6: Testing moisture resistance in part ...
Sean Member

Ok, I found EN 318 might have something to do with it. Its a European standard that tests changes in dimensions due to moisture. I am not sure if there is an equivalent ANSI standard.

Anyway, this may be what I'm looking for.

3/5/13       #7: Testing moisture resistance in part ...
Alan F.

Sean,
It looks like this may already be tested, we have used this for exterior trim and fascias

MEDEX Specs

3/31/13       #8: Testing moisture resistance in part ...
Jan Oostland  Member

Website: http://www.maximasa.com

I have never seen Particle board that is truly moisture resistant. MR particleboard can stand up against an occasional splash better then regular. You can easily do your own test. Set a piece of 2" x 2" Regular Particle Board next to a same size piece of MR Particle board on edge in a dish of water. Fill the dish with like 1/8" of water and watch the results. The MR will swell up but at a much slower rate the first hour. After about 24 hours they might be swollen the same amount. Now you can probably decide if Particle Board is the right material for your project.

4/10/13       #9: Testing moisture resistance in part ...
Rich  Member

Website: http://www.hausmann.com

MR particle board is not that uncomon we use it when requested (Medex is one that we have used). We usualy get requests to use on countertops that have sinks. If you take a look on the particle board manufacture sites there will be the specs on each type of board (probably no need to have tested). Also the board usualy has a dye added during manufactur so you can identify the difference types (I think MR is green and fire rated is red).

Depending on the specs for the job you may need to use special glue. If you are using a PVA some manufactures have a catalist to make the glue moisture resistant.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Excel Wood Products