HolzHer Edgbander Glue problems
12/2/14
HolzHer Edgbander does not extrude glue out of the bottom 2 to 3 holes. Any tricks for PERMANENTLY fixing this. I have removed dosing rod many times and cleaned out entire rod and holes. I have used different glues and temps but always end up with this problem. Time to replace a part? Machine is 10 years old. Help!!
12/31/14 #2: HolzHer Edgbander Glue problems ...
Website: http://www.weinig.com/en/panel-processing/holzher-...
The best practice is to always call our tech support line first 704-587-3400. By calling in your questions and issues are logged for future reference to your problem.
They're few parts to our glue system. Typically long term wear items are dosing rods and heaters. Our guy's will get you straightened out.
12/31/14 #3: HolzHer Edgbander Glue problems ...
You may have contaminates still in the glue station that re-plug the holes after you remove the dosing rod and poke out the holes. You can try leaving the dosing rod out and turning on the glue station and flushing the glue and contaminates out of the empty dosing rod hole. Just use a piece of cardboard or something to divert the flushed out glue over the front of the nozzle so that glue doesn't go everywhere and make a mess.