Subject: Re: Exterior use of Sapele

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Exterior use of Sapele

5/15/22       
Marcelo

Plan on sheathing an exterior (NC, fully exposed) kitchen cabinet with Sapele (purchased as KD 3/4 S4S, random widths). Cabinet is ~ 105"Lx25"Dx33"H rectangular prism with 4 doors & 2 drawers, on one long side. Built upon a construction 2x4 skeleton. How do I deal with Sapele's expansion/shrinkage or tendency to cup? Vertical boards, or horizontal best? For the 105"x33" rectangle, horizontal may be better??? Maybe fixed screws (SS) at top where they will be hidden by granite counter overhand and then use Z clips (not iron) attached to the vertical 2x4 skeleton connected the back of the Sapele (one per board, centered) to allow downward movement (lateral expansion) and still keep it flat (at 3/4 S4S, screws would be short!). The 100x33" rectangle would be boards glued together so it moves as one without creating gaps. The sides, 25x33" could be done similarly or with vertical boards. Again, gluing together would allow it to move as one piece. If I glue these myself I could use buiscuits... Regular exterior glue good enough? I read mixed inputs on the gluability of Sapele, cabinet corners could be 5/4 or 6/4 moldeed to overlap the main panels so some expansion contraction could be hidden... was going to use Ipe for this but its 3X the cost. Ideas, suggestions, recomendations and cautionary tales welcomed. Assume finish will be some sort of recomended exterior UV shielding oil. Should this project be successful, 24' of benches to follow, large table... and more. As I am sure all readers can tell, this is an amateur asking! Thank you in advance for your assistance!

5/19/22       #3: Exterior use of Sapele ...
David R Sochar Member

Why would you build a box out of 2x4 and then
clad it with a fine hardwood? The Sapele is perfectly capable of being both the structure and the face.

Or perhaps I am just not understanding your cabinet/plan. A drawing or two would be helpful to address your concerns with movement.

5/19/22       #4: Exterior use of Sapele ...
David R Sochar Member

Well, just absorbed the "amateur asking" statement.

'Zacktly how does an amateur get the amount of high end (?) work you mention?

Benches and tables - you are a long way from being able to design the production of such things, are you not?

5/19/22       #5: Exterior use of Sapele ...
RichC

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.

5/19/22       #6: Exterior use of Sapele ...
Marcelo Member

Apologize, did not realize I could not ask questions from an amateur perspective. This is something I am doing for myself. I can provide drawings, but I guess it would be inapropriate for me to do so. I am located in NC, Raleigh area if anybody cares to contact me directly. I realize what I am planning is not "normal" which is why I was hoping for a higher caliber of help.

But, to answer the question, agree I could use the same wood for the frame, but I do not see that as needed.

I enjoyed reading the blog between professionals. Very enlightning.

Thank you for reading my question and sorry for wasting your time.

5/19/22       #7: Exterior use of Sapele ...
pat gilbert

Dave, Rich objects to to you stealing his rice bowl

5/20/22       #8: Exterior use of Sapele ...
Adam B Member

Once again, I just don't get it. Our industry, along with every other trade profession out there is struggling/desperate to find anyone that may be interested in what we do. Instead of helping or teaching those that actually show some interest, there is a group on this site whose sole purpose is to try and maintain some sort of "holier than thou" mentality as if they are too important or qualified to help resolve a serious issue facing our industry. Why not use our time and effort to help build up interest in what we do, instead of continually berating and alienating those that actually show some sort of interest? The potential ROI could be exponentially more than we can even imagine.

Marcelo, on behalf of the reasonable people on this site, I would like to offer an apology for the responses you have received thus far. I have been in the wood working industry for 30+ years, but unfortunately I have not had the opportunity to focus/work on exterior cabinetry to the point that I can offer confident advice. I actually built myself something very similar to what you are describing for my own personal use on my deck. The big difference is I wrapped the frame structure in composite decking material to match my newly built deck.

Hopefully someone with some exterior woodworking experience can chime in and actually give you some sound advice, best of luck with your project.

5/20/22       #9: Exterior use of Sapele ...
Marcelo Member


Thank you, reasonable thing to do! I thought of it, my wife disaproved!

Will explore if I can get the boards shiplapped milled. May be the better part of valor. More straightforward to address potential for expansion and cupping. which is my only real concern. All else I can do, albeit not efficiently, but that is not the point for me.

Nevertheles, time is $ and I do not waste folks time.

Thank you again.

5/20/22       #10: Exterior use of Sapele ...
David R Sochar Member

Website: http://www.acornwoodworks.com

The forum rules set the tone for helping people without a professional shop. Not so much a holier than thou as it is just against the guidelines that site owners/administrators have set up. They pay for this site to exist.

I suggest Marcelo be sent elsewhere, where he can get good help and advice. I also suggest he post good sectional drawings showing how he proposes to build this cabinet. While he may feel his explanation is adequate, it is only as it comes from his perspective. Drawings are the language we communicate with, so that is where we stand.

5/20/22       #11: Exterior use of Sapele ...
Marcelo Member

Decided to add a graphic and specifications since it was mentioned. Excluded the frame details as that is my approach which I am sure nobody else would use. Intent is to maximimize internal useful space and not waste it on supporting structure, as much as practicably possible. A lot of drawers trying to maximize useful width of each.


Click the link below to download the file included with this post.

Outdoor_wood_kitchen_detailed__Ext_Drwg_Rev01.pdf

5/21/22       #12: Exterior use of Sapele ...
Robert Member

If 85% of what RichC posts is inappropriate and basically useless I say we help Marcelo with what looks like a very interesting project.

5/21/22       #13: Exterior use of Sapele ...
pat gilbert

Nope, RichC and Dave's post are very useful

5/22/22       #14: Exterior use of Sapele ...
Jim

To maximize space I'd use 3/4" 2 sided MDO exterior plywood for the case including the back, lumber edgebanding, then clad with frame and panels of your choice or shiplapped vertical or horizontal boards, allowing for some inevitabe movement

5/23/22       #15: Exterior use of Sapele ...
Marcelo Member


Thank you Jim. Will explore your suggestion.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!