Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Edgebanders are hard!

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Edgebanders are hard!

2/2/19       
Riley Member

I am not new to edge banding, but I am new to edgebanders!

After a few near tears moments, a few thrown wrenches and lots of cursing the italians outloud - I have finally mostly dialed in this wild mustang of a machine.

As with my CNC everything will be going along happy clappy most of the time and then in .2 seconds goes to hell.

For starters let me just say ask again for the record - why can't anyone make a decent manual? I mean seriously I end up having to make a comprehensive second manual for just about every machine I purchase. This one takes the cake. It basically says - Insert Tape somewhere, don't forget to add glue sometimes, good luck! (The parts diagram is very solid however, only missing sizes and threads for the parts - but everything else is well documented)

Ok tantrum over.

My Questions -

My machine (SCM K208 E) has a Cut off Saw, Tiltable Edge Bevelers, Glue Scraping Unit, Buffers.

We only use 5/8 and 3/4 Pre-Finished Birch. We are using 7/8 pre-finished edgebanding.

1. We are using the 7/8 banding for both sizes of plywood - is that okay? Sometimes the front edge of the panel gets a bit "torn" on the top corner from the cut off saw - I am wondering if this is because either the blade needs sharpening, or material is too tall without support when the saw comes down to chop it off.

2. Is the scraping unit only for PVC? It has a radius R3 on the "plate" (what I would call the scraper) and the manual only references PVC when speaking about adjustments for this unit. I tried adjusting it as much as I could to get a clean edge but then had the idea to just take them off and low and behold had a much better edge when the unit was omitted. Is this something that I could order a different plate for - or is this only used in PVC edge banding to knock down the corner on it and I should just keep it off?

3. The buffing wheels need to be replaced as they are old. Does anyone have a recommendation on what type to replace them with for our purpose?

4. The buffing wheels can be angled, does anyone have a recommendation on what angle to run them at.

5. The yellowish glue we are using is coming out a dark brown on the gluing unit. The machine suggests 200c - but is our temperature too high and the brown is a sign of that - or - is our unit dirty and needs to be cleaned?

6. What can I expect for the accuracy of an edgebander? Right now, one in every 20 or so pieces has some kind of issue with it - usually its the front edge is a bit torn. I notice that a lot of the newer units have a mill on the front that lets you take the banding off and rerun it - so I am wondering if this is just a common reality of edgebanders along the lines of the occasional small parts moving on my nested router when the spoil board is beat up.

Any help would be greatly appreciated!

Thanks!

2/2/19       #2: Edgebanders are hard! ...
Luke Vickery

1. I'd suggest not using 7/8 edgebanding on 5/8 material. Try cutting 20' of edgebanding to 3/4 and run it on 5/8 material.

2. Only used for PVC. The 3R denotes 3mm radius. It is designed to scrape 3mm PVC. Don't use your scrapers for wood.

3. I would suggest contacting SCM for replacement parts - partspronto@scmgroup.com

4. Trial and error for the buffing wheels. They are probably oscillating so maybe a15-degree angle depending on how worn they are.

5. I would recommend a good clean and checking the suggested temp via the glue mfr.

6. You should expect high accuracy for an edgebander. It requires a lot of practice and fine adjustments. If the front edge is torn, it could be that your edgebanding is too wide for the material - 7/8" edgebanding on 5/8" material is a problem. Also, check all of your tooling. Dull blades, scrapers, etc. deliver poor results.

Good luck!

2/2/19       #3: Edgebanders are hard! ...
cabinetmaker

20 degree on the edge bevelers

Call parts at scmi with serial number and model for the buffers.

Need to mage sure your blades are sharp and aligned with the tracer or shoe for a good clean flush cut.

Keep the glue low enough to use up what you put in vs always topping off. Glue will go bad sitting in the pot cooking.

Banders are easy.

2/3/19       #4: Edgebanders are hard! ...
uselessinformation77

We use a SCMI, when it runs great im a happy worker, but look out if it acts up. We were getting chips on the front of our material. I came to the conclusion that the feed roller and pressure feed rollers,were adjusted to far towards the outside of machine. They were actually folding the front piece of laminate just enough to give it a hairline split. then which the cut off blade would chip when it came down to cut.

2/3/19       #5: Edgebanders are hard! ...
Hen Bob Member

We have set up a few used edgebanders over the years. As the others have said start with all new cutters and buffing wheels. We also had the tech come out for a day and make sure everything was right once it was up and running.

Money well spent

2/4/19       #6: Edgebanders are hard! ...
matt

A couple points:

Buffing wheels not needed for prefinished wood edgebanding. It's mostly for PVC. If you're using buffing wheels with prefin wood, what your'e really doing is using the buffing wheels to clean off glue, which is not a good thing. Eventually you'll end up with smears. Turn the buffers OFF and get them out of the way.

You may have a glue scraper. Obviously you don't need your 3mm radius "Profile scraper", that's for PVC/plastic EB only. But it's up to you whether you use a glue scraper with prefin ply and PVC edgeband. I personally would not use it if I'm using prefin wood edgeband, but I could be talked into it. I do not ever use it on raw plywood though.

Glue temp---- you need to stick to the glue temp range given by your glue manufacturer. I've found with all 3 of the edgebanders I've ever touched that winter time = use the upper range of their temp, and summer= use the lower range. Especially with gluepot machines. I've not found cartridge machines (like Holz-Her) to be all that sensitive.

My edgeband pellets sit in a LIDDED plastic rubberbaid garbage can next to the machine. Over the top of that can, on the wall, is a plastic pouch with the glue MSDS and "Information" sheet, so that there is never a question as to what glue I want in that bander, and where to find information on it.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello