Using FRP in cabinet

12/30/19       
Garen

I have a client looking to use FRP inside of the cabinet over the laminate and corners caulked. Has anyone done this or have any other ideas. Looking for a water proof interior for sink cabinets.

12/30/19       #2: Using FRP in cabinet ...
Garen

Also can FRP be applied with contacted adhesve to a moisture resistant MDF.

12/31/19       #3: Using FRP in cabinet ...
Adam

Explain more in detail what the are the clients needs. frp is fibreglass reinforces plastic. It’s typically applied with dry fibres and wet resin. Like on a boat.

12/31/19       #4: Using FRP in cabinet ...
cabinetmaker

Yes.

Went to the local box store and lined the bottom first. Then added the back and sides.

Used 3.0 quick grab (I think). Glued right to melamine.

Did not come off. Soda cabinets. Cut around the hinges.

12/31/19       #5: Using FRP in cabinet ...
Tom Gardiner

Wouldn't HPL provide the same moisture resistance? The difference isin the caulked joints. It would be a whole lot easier to work with.

12/31/19       #6: Using FRP in cabinet ...
Garen Pletzer

They want to make sure to stay water tight. They have been back to some jobs that have had the bottoms damaged. Not my cabinets so i want to make sure I do a good job and make this not get water logged. Its a restaurant and they will put buckets of water under there and enything you can think of. I thought about using a thru color laminate. I looks like it has a different backing. If the FRP sticks to the laminate i think i would rather do that. I found I can get it layid up but that makes it pretty thick on 3/4" material with only being able to get it double sided. The FRP is used a lot in restaurants in the back and areas of high wear. Where possible water could be. When I was doing countertops for MCDS it was all over the whole kitchen and under the countertops.

12/31/19       #7: Using FRP in cabinet ...
Garen Pletzer

Tom- I did mention that to the contractor that its possible they also used a cheap melamine and with it not being caulked it would just run down and the partical board would just suck it up. I am trying to get more info on how the thru color laminates are made and if they would be more moisture resistant with it looking like it has a different backer and then put on a medex. Then caulk the sides with a good caulk.

12/31/19       #8: Using FRP in cabinet ...
MarkB Member

Why not make the decks out of Starboard? Or even PVC sheet stock, Azek, Permatrim, Royal?

12/31/19       #9: Using FRP in cabinet ...
Ex-Pat Member

I think Mark is really on the right track with some sort of solid core. You can use as much FRP and caulking as you want, as soon as someone punches a hole for plumbing you've got a problem. Of course, the cost may be prohibitive. But to answer your question, in my experience yes FRP can be contacted to a moisture resistant MDF. I've done it before and not had it fail.

12/31/19       #10: Using FRP in cabinet ...
Alan F.

We see this in commercial cabinets in kitchens and break rooms with lots us use, usually at open sink cabinets and appliance bays. We have it cold pressed like laminate.

Generally the specs use the same stuff on the cabinet back that is going on the walls.

If you want to build a water resistant cabinet use metal or compact laminate.

A-

Click the link below to download the file included with this post.

sample1231.pdf

1/1/20       #11: Using FRP in cabinet ...
cabinetmaker

as an alternative we use medex with VG PL pressed with interior color but it's all the same, clients letting maintenance lapse due to failure of scheduling inspections

Seems that more sink bases here in the Midwest are leaning to sloped panels with no floor

We started making them as unit as the carpenters would lose the false fronts and not hold the dimensions for a top properly


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello