RT Machine Co

CNC

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Biesse/Microvellum code error

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Biesse/Microvellum code error

1/27/15       
Steven

Hello everyone,

We have a Biesse/Microvellum setup and there has been a problem that has surfaced recently. The router cuts the outside profile and then right before it leads out it dips into the part. Sometimes we can work around it but many times I have to re-cut manually. Anyone had this issue in this configuration? Your help is much appreciated.


View higher quality, full size image (1456 X 2592)

1/27/15       #2: Biesse/Microvellum code error ...
cabinetmaker

Look @ the post right as you get to G40 turning off correction and see what the last lines of code are doing.

High light the program and hit "Edit" should be able to draw and watch the last step even if sent via Microvellum.

Have you upgraded software lately ? or have you copied the program you are using currently, over and over ?

1/27/15       #3: Biesse/Microvellum code error ...
STEVEN

I have the updates. I have copied the machining lines over and over but the error happens on parts that have no machining.

1/27/15       #4: Biesse/Microvellum code error ...
cabinetmaker

We had kind of the same problem when checking the post with the machine during integration. We ran it several times to get the post just right. I do not have Microvellum, but our post from the software had to be integrated with the NC 1000 integral Biesse post.

Find an old program that is not doing this and analyze the last three or four lines ? Are you squaring off you nest ? Did you just recently stop this ?

1/27/15       #5: Biesse/Microvellum code error ...
Steven

Ill find an old part and compare.

I dont square the nest, never had to.

Havent stopped it yet.

1/27/15       #6: Biesse/Microvellum code error ...
alien Member

Is this a nested part because it looks like a lead in or out from an adjacent part?

1/28/15       #7: Biesse/Microvellum code error ...
STEVEN

It is a nested part and it does seem to be related to the lead out but It only becomes noticeable after microvellum converts the machining.

1/28/15       #8: Biesse/Microvellum code error ...
Alien Member

Have you changed bit size or Space between panels? Go to tool file under nesting tab and read over the values. I will look on mine and see if anything pops out. What machine is it? V6.7 or v7

1/28/15       #9: Biesse/Microvellum code error ...
cabinetmaker

you are going o have to look @ the last lines of code of a good posted nest and the bad. This will give you the insight you need

1/28/15       #10: Biesse/Microvellum code error ...
Alien Member

This is my nest settings


View higher quality, full size image (2048 X 1152)

1/28/15       #11: Biesse/Microvellum code error ...
STEVEN

The part spacing is good, my settings are much the same Im trying to examine the code but taking me some time. Im not familiar with this method

1/28/15       #12: Biesse/Microvellum code error ...
Frank D. Jimenez  Member

Website: http://www.cabinetpro.com

Is your CNC setup within MV writing to Biesseworks, or is it writing raw g-code? There MAY be a variable within the code telling the spindle to lead in to the material, or lead out of the material, as though the cut was a curve rather than a straight dado.

1/29/15       #13: Biesse/Microvellum code error ...
STEVEN

It is writing to biesseworks

1/30/15       #14: Biesse/Microvellum code error ...
Brian

Had to do a double take on that screen shot haven't seen that tab for a day or two, they have added and change it a bit. but what I see is what I use. Yep look at the code, the machine is only doing what it is told.

1/30/15       #15: Biesse/Microvellum code error ...
cabinetmaker

Open the editor on that program in Biesseworks and hit the draw symbol watch for the end of the tool path. If it is veering off at the end then you are having a mis-interpretation between microvellum and the Biesse post. ??

Your original post said that it is a recent devopement. You need to go back and figure out what happened between then and now.

You are also saying it does not happen with parts that are not machined. Yes that is what we understand. I see that you have stated that it happens with copying line after line. Ok. Does it happen with a fresh drawing. As new. Not a copied one. ??

1/31/15       #16: Biesse/Microvellum code error ...
dylan

Website: http://www.cnc-tool.com

is the file a .cix / .iso / .dat

I suspect as stated in previous posts the problem is lead in/out setting.MV may be sending through the post a helical lead in or out and with the data in your offset, leaving the tab.
post or email to me a screen shot of the milling data of the tool creating the problem, assuming its a .cix file.
as always service@biesseamerica.com is avail.

regards
dylan bayliss
www.machineconsult.com

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA Limtech Industries, Inc.