Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: 2K poly

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

2K poly

5/7/19       
Thomas

Hello,
We are having problems finding a quality 2k poly. We used Mohawk up to the point that it was discontinued. We have tried Chemcraft Verde, which did not work for us. What other companies have a quality product. What are others using with good results? Thanks
Thomas

5/7/19       #2: 2K poly ...
chris

I use Ilva products from camger coatings.

5/7/19       #3: 2K poly ...
dean c

ILVA

ICA

5/7/19       #4: 2K poly ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

We use ICA. All kinds of choices for 2K PU

5/7/19       #5: 2K poly ...
Leo G Member

MLC Polarion

Milesi

5/8/19       #6: 2K poly ...
CraigM

Another vote for Milesi

5/8/19       #7: 2K poly ...
Thomas

Website: http://hitefieldwoodworks.com

Thanks for the responses. Leo, we have tried Polarion or at least had a rep show it to us. One of the contributing factors for the new product will be tech support and availability,
Craig, I have not seen Milesi but have now looked at their website. They look promising. When Mohawk quit the 2k we decided not to use it and just shoot lacquers and c/v....but some products really need the 2k.
Thanks again for the help.

5/8/19       #8: 2K poly ...
Leo G Member

Atlantic Plywood is where I get my finishes. They carry both the MLC Polarion and the Milesi 2K products. So you have a two fer if you have an Atl Ply by you.

5/8/19       #9: 2K poly ...
Brian Member

Sirca from Gemini

5/8/19       #10: 2K poly ...
mauricio poli Member

My vote is for Sirca-Gemini
Ask also for Water Based 2 K samples, it is very good.

5/8/19       #11: 2K poly ...
Kevin Member

Mind if I ask what you did not like about the verde?

5/9/19       #12: 2K poly ...
Thomas

Kevin
We could not get the verde to lay right. When mixed according to the specs, it would dry to touch in less than three minutes. We kept adjusting the mix till we were double the retarder and three times the amount suggested for reducer. Still would dry so fast that the passes would not burn in. Attempted to contact tech support numerous times and eventually learned that AkzoNobel has no tech support. So, we are still looking for a replacement.

5/9/19       #13: 2K poly ...
JaySun

MLC has an Alkyd/Acrylic hybrid product now called Coda. 10:1 mix ratio up to 4 hour pot life. Sprays good and sands well. With it being a hybrid it does have amber look.

5/9/19       #14: 2K poly ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

Well I think almost every brand has been listed.
What you need to do is call the local or nearby Dist and have them come out and demo the products you are interested in.

All PU's are not equal, they spray different, lay down differently, feel and look different and tech support is different.
Tech support is big, both in person or somebody available by phone for questions.
PU's are a technical product.
Start making some calls and see who responds, that's where the service starts.

5/20/19       #15: 2K poly ...
Gary

I just tried a 2 part Polly from Campbell it's called Coda, I was very impressed, sprayys out real nice and looks great !

5/30/19       #16: 2K poly ...
Ed

Melisi. I’ve sprayed, Polarion, coda, Ora verde and still, Melisi is my all time favorite. Others make it easy by having one catalyst for everything, but it’s really not that difficult. This is furniture grade finish in a multitude of sheens. Interior/exterior.

5/31/19       #17: 2K poly ...
Thomas

Thanks all for the responses. Milesi is sending a rep out Tuesday morning. I hope it works out for us.

7/26/19       #18: 2K poly ...
Jeff

ML Campbell CODA is amazing! Contact your local distributor to try it out!

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)